Evidence map›Paper›PMID 42593826›Full record

ArticleAdvanced science (Weinheim, Baden-Wurttemberg, Germany)2026

Further Evidences for the Sulfur Spillover on Carbon: Thermodynamic Aspects and Effects on Li-S Solid-State Batteries.

Francesco Piccolo, Anka Berger, Sebastian Risse, Román Healy Corominas, Wilhelm Erth, Florian Fuchs, Jesus Andrade, Jörg Schuster, Marc Armbrüster, Philipp Adelhelm

Abstract read
In one paragraph

Article in Advanced science (Weinheim, Baden-Wurttemberg, Germany), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

10 authors.

Francesco PiccoloInstitute of Chemistry, Humboldt-Universität zu Berlin, Berlin, Germany.
Anka BergerBAM, Bundesanstalt für Materialforschung und -prüfung, Berlin, Germany.
Sebastian RisseResearch Group Operando Battery Analysis (CE-GOBA), Helmholtz-Zentrum Berlin für Materialien und Energie (HZB), Berlin, Germany.ORCID https://orcid.org/0000-0003-0100-8365
Román Healy CorominasInstitute of Chemistry, Humboldt-Universität zu Berlin, Berlin, Germany.ORCID https://orcid.org/0009-0004-7517-1338
Wilhelm ErthInorganic Solid State and Material Chemistry, Eduard-Zintl-Institute, Technical University Darmstadt, Darmstadt, Germany.ORCID https://orcid.org/0009-0006-3594-1021
Florian FuchsChemnitz University of Technology, Chemnitz, Germany.ORCID https://orcid.org/0000-0003-2886-9835
Jesus AndradeInstitute of Chemistry, Materials for Innovative Energy Concepts, Chemnitz University of Technology, Chemnitz, Germany.ORCID https://orcid.org/0009-0009-2606-5236
Jörg SchusterChemnitz University of Technology, Chemnitz, Germany.
Marc ArmbrüsterInorganic Solid State and Material Chemistry, Eduard-Zintl-Institute, Technical University Darmstadt, Darmstadt, Germany.ORCID https://orcid.org/0000-0002-2914-0600
Philipp AdelhelmInstitute of Chemistry, Humboldt-Universität zu Berlin, Berlin, Germany.ORCID https://orcid.org/0000-0003-2439-8802

Funding

Berlin Battery LabBundesanstalt für Materialforschung und -PrüfungDeutsche Forschungsgemeinschaft 517014885Helmholtz-Zentrum Berlin für Materialien und EnergieHumboldt-University Berlin
6 · The paper itself

Abstract

This study investigates sulfur spillover, the spontaneous and rapid spread of sulfur over carbon surfaces at ambient temperature. The process is studied by small-angle X-ray scattering (SAXS), X-ray radiography, and microcalorimetry from which a number of physicochemical properties are derived. The results confirm that sulfur immediately interacts with porous carbon upon mixing, with most signal changes occurring within a few hours. For the first time, thermodynamic data of the process are determined. Using microcalorimetry, the lower bound of the reaction enthalpy is determined to be Δ

Indexed as

activated carbonLi‐S batteriessolid‐solid adsorptionsolid‐solid wettingsulfursulfur‐carbon compositessulfur spillover

Identifiers

PMID42593826
PMCPMC13472108

What OpenQuestion holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.