Coherent Solid-Solution Interface With Near-Zero Lattice Mismatch Enables Stable Zinc Anodes.
Article in Advanced materials (Deerfield Beach, Fla.), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
13 authors.
Funding
Abstract
Aqueous Zn-ion batteries (AZIBs) are attractive for large-scale energy storage owing to their high theoretical capacity, intrinsic safety, and low cost. However, interfacial instability of Zn metal remains a major obstacle, leading to dendritic growth, parasitic reactions, and rapid capacity decay. Here, we introduce a coherent solid-solution interface (SSI) strategy with near-zero lattice mismatch to stabilize the Zn metal anode. The in situ formed SSI exhibits a lattice mismatch of only 0.11% with Zn, enabling coherent Zn growth and suppressing detrimental side reactions. Combined experimental and theoretical analyses reveal that the SSI reduces interfacial polarization, suppresses HER, and promotes uniform lattice-aligned dense Zn deposition. As a result, SSI-Zn delivers stable Zn||Zn symmetric cell cycling for over 9100 h (1 year and 18 days) and achieves Zn||Cu asymmetric cell performance with a Coulombic efficiency (CE) of 99.9% over 10 000 cycles. In full cell configurations, Zn||AC cells and Zn||I