Evidence map›Paper›PMID 42589858›Full record

ArticlePolymers2026

Thermal Depolymerization Challenges of PTFE:Silicone Rubber Mixtures and Composite Materials.

Lukas Eigenschink, Matthias Mastalir, Michael Harasek, Christian Paulik

Abstract read
In one paragraph

Article in Polymers, 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors.

Lukas EigenschinkInstitute for Chemical Technology of Organic Materials, Johannes Kepler University Linz, Altenberger Straße 69, 4040 Linz, Austria.ORCID 0009-0000-1487-1817
Matthias MastalirOMV Downstream GmbH, Mannswörther Straße 28, 2320 Schwechat, Austria.
Michael HarasekInstitute of Chemical, Environmental and Bioscience Engineering, TU Wien, Getreidemarkt 9/166, 1060 Vienna, Austria.ORCID 0000-0002-6490-5840
Christian PaulikInstitute for Chemical Technology of Organic Materials, Johannes Kepler University Linz, Altenberger Straße 69, 4040 Linz, Austria.ORCID 0000-0002-1177-1527

Funding

OMV (Austria)
6 · The paper itself

Abstract

Thermochemical depolymerization of polymer mixtures and composite materials is challenging due to non-additive degradation behavior and the emergence of new reaction pathways during pyrolysis. Both polytetrafluoroethylene (PTFE) and silicone rubber (SR) can depolymerize into monomers or low-molecular-weight oligomers when pyrolyzed individually, making them, in principle, suitable candidates for depolymerization-based recycling. Because they are frequently combined in technical applications and composites, their behavior during co-pyrolysis warrants investigation. However, the pyrolysis of PTFE:SR mixtures and composites remains poorly understood. In this study, we examine the pyrolysis behavior of PTFE:SR systems with emphasis on mass balance, product composition, and the formation of new species to address potential limitations for depolymerization-based recycling. Experiments were conducted on virgin PTFE and SR, defined polymer mixtures, and commercially relevant composites, including PTFE-lined silicone tubing and PTFE:SR septa. The results reveal a pronounced, non-linear dependence of product distribution on PTFE content. Product identification by GC-MS, NMR, and FTIR indicates cleavage of Si-O and Si-CH

Indexed as

co-pyrolysisdepolymerizationPFASPTFEsilicone rubberthermal recycling

Identifiers

PMID42589858
PMCPMC13468768

What OpenQuestion holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.