ArticleMaterials (Basel, Switzerland)2026
Effect of Chloride Concentration on the Corrosion Behavior of an Iron-Based Amorphous Coating and 316L Stainless Steel in Saline Soil from Daqing.
Article in Materials (Basel, Switzerland), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
3 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
AISI 316L stainless steel (316L SS) exhibits inadequate corrosion resistance in chloride-containing soils. Fe-based amorphous coatings (Fe-ACs), owing to their high Cr, Mo, and W contents and defect-free amorphous structure, are promising candidates for superior protection. In this work, the corrosion behavior of 316L SS and an Fe-based amorphous coating (Fe-AC) fabricated by high-velocity oxygen-fuel (HVOF) spraying was systematically compared by burial in Daqing saline soil (25% water content) with 0, 1.0, and 2.0 wt.% NaCl for 15-55 days. Corrosion rates were measured via mass loss, and surface morphology, elemental distribution, and phase constitution were characterized using OM, SEM/EDS, and XRD. Electrochemical impedance spectroscopy and potentiodynamic polarization were employed to assess passive-film stability and charge-transfer resistance. The Fe-AC consistently exhibited an extremely low corrosion rate (below 0.01 mm y
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.