ArticleBioengineering (Basel, Switzerland)2026
Mechanical Behavior of Conventional and Subtractively Manufactured Dental Resin Composites After Water Degradation.
Article in Bioengineering (Basel, Switzerland), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
- Evaluation of Fracture Resistance in CAD-CAM Additively Manufactured Occlusal Veneers.Polymers · 2026Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
7 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The ongoing development of subtractive options for indirect restorations places clinicians in a position that requires adaptation, understanding and choosing of the most suitable option for the long-term survival of the restoration. Mechanical parameters represent important indicators of long-term success. Consequently, this research aimed to assess the impact of water sorption on the mechanical properties of two direct resin composites, Gradia Direct Anterior A2 and Filtek Z550 A2 and three CAD/CAM subtractively manufactured dental resin composites, Vita Enamic, Brilliant and Cerasmart. A total of one hundred specimens (50 control, 50 underwent this protocol: dehydration, immersion in distilled water for 30 days and then re-desiccation), standardized to the dimensions of 14 mm × 4 mm × 1.2 mm were subjected to three-point bending test (based on ISO 4049:2019 and ISO 6872:2015), in order to find out the flexural strength and the elastic modulus of the material at the breaking point. Then, the fractured sample surfaces were fractographical analyzed. Using the two-parameter Weibull approach, the Weibull modulus (m) and the characteristic strength (σ
Indexed as
Identifiers
What OpenQuestion holds
Registered trials