Evidence map›Paper›PMID 42390888›Full record

ArticleAngewandte Chemie (International ed. in English)2026

Chloride-Regulated Depolymerization of Aluminosilicate Networks for Fast Ion Transport Compliant Interfaces in Sustainable All-Solid-State Sodium Batteries.

Liyu Zhou, Xingyu Wang, Rui Yang, Yang Xu, Simeng Zhang, Meng Li, Han Wu, Xinmiao Wang, Junyi Yue, Yueyue Wang and 12 more

Abstract read
In one paragraph

Article in Angewandte Chemie (International ed. in English), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

22 authors.

Liyu ZhouDepartment of Applied Chemistry, School of Chemistry and Materials Science, University of Science and Technology of China, Hefei, China.
Xingyu WangEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Rui YangAdvanced Energy Storage Technology Research Center, Shenzhen Institute of Advanced Technology, Chinese Academy of Sciences, Shenzhen, China.
Yang XuDepartment of Applied Chemistry, School of Chemistry and Materials Science, University of Science and Technology of China, Hefei, China.
Simeng ZhangEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Meng LiSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Han WuEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Xinmiao WangEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Junyi YueEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Yueyue WangSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Huaimin JinEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Xiangzhen ZhuEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Mingying ZhangEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Chenxiang LiSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Xuan YangSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Xiaoyang YuanSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Wen YinInstitute of High Energy Physics, Chinese Academy of Sciences (CAS), Beijing, China.
Wei XiaEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.
Changtai ZhaoSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.
Jianwen LiangSolid State Batteries Research Center, GRINM (Guangdong) Institute for Advanced Materials and Technology, Foshan Key Laboratory of Advanced Electrochemical Functional Materials and Technology, Foshan, China.ORCID https://orcid.org/0000-0003-4055-1301
Xueliang SunEastern Institute for Advanced Study, Zhejiang Key Laboratory of All-Solid-State Battery, Ningbo Key Laboratory of All-Solid-State Battery, Eastern Institute of Technology, Ningbo Institute of Digital Twin, Ningbo, China.ORCID https://orcid.org/0000-0003-0374-1245
Xiaona LiDepartment of Applied Chemistry, School of Chemistry and Materials Science, University of Science and Technology of China, Hefei, China.ORCID https://orcid.org/0000-0001-6713-2997

Funding

Commanding Heights of Science and Technology of Chinese Academy of Sciences LDES150000National Key R&D Program of China 2025YFF0523000National Natural Science Foundation of China 22379127National Natural Science Foundation of China 52472127National Natural Science Foundation of China U25A20627National Natural Science Foundation of China W2441017Ningbo Yongjiang Talent Introduction Program 2023A-184-GZhejiang Provincial Natural Science Foundation of China LR26E020002
6 · The paper itself

Abstract

All-solid-state sodium-ion batteries (ASSSIBs) provide a sustainable and cost-effective solution for large-scale energy storage. Sodium aluminosilicate (NASO) represents a resource-sustainable electrolyte option owing to their low cost, natural abundance, and electrochemical stability. However, their strong covalent network leads to intrinsic low ionic conductivity, and poor interfacial compatibility. This work employs Cl incorporation to depolymerize the hyperconnected covalent network of NASO, forming a modified NaAlSiOCl (NASOC) structure with discrete short-chain segments, which turns stress-induced large-scale cooperative rearrangement into localized deformation. Replacing a strong O─bridge with a weaker Cl─bridge further reduces the Young's modulus. Additionally, chloride doping effectively reduces the Na

Indexed as

all‐solid‐state batterieshalide solid electrolyteinorganic depolymerizationsodium aluminosilicateYoung's modulus

Identifiers

PMID42390888
PMCPMC13528543

What OpenQuestion holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.