Evidence map›Paper›PMID 42376776›Full record

ArticleAngewandte Chemie (International ed. in English)2026

Adsorption-Mediated Sodium Compensation for Hard Carbon Anodes Enabled by Soft-Contact Presodiation.

Shuai-Qi Wang, Yi Yang, Yao-Peng Chen, Chong Yan, Xue-Kun Cao, Zhou-Qing Xue, Hao Wang, Qian-Rui Zhao, Xiang Chen, Jia-Qi Huang and 1 more

Abstract read
In one paragraph

Article in Angewandte Chemie (International ed. in English), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

11 authors.

Shuai-Qi WangBeijing Key Laboratory of Complex Solid State Batteries, Department of Chemical Engineering, Tsinghua University, Beijing, P. R. China.ORCID https://orcid.org/0009-0005-4573-6470
Yi YangSchool of Interdisciplinary Science, Beijing Institute of Technology, Beijing, P. R. China.
Yao-Peng ChenBeijing Key Laboratory of Complex Solid State Batteries, Department of Chemical Engineering, Tsinghua University, Beijing, P. R. China.
Chong YanSchool of Interdisciplinary Science, Beijing Institute of Technology, Beijing, P. R. China.ORCID https://orcid.org/0000-0001-9521-4981
Xue-Kun CaoShanxi Research Institute For Clean Energy, Tsinghua University, Taiyuan, P.R. China.
Zhou-Qing XueSchool of Interdisciplinary Science, Beijing Institute of Technology, Beijing, P. R. China.
Hao WangSchool of Interdisciplinary Science, Beijing Institute of Technology, Beijing, P. R. China.
Qian-Rui ZhaoShanxi Research Institute For Clean Energy, Tsinghua University, Taiyuan, P.R. China.
Xiang ChenBeijing Key Laboratory of Complex Solid State Batteries, Department of Chemical Engineering, Tsinghua University, Beijing, P. R. China.ORCID https://orcid.org/0000-0002-7686-6308
Jia-Qi HuangSchool of Interdisciplinary Science, Beijing Institute of Technology, Beijing, P. R. China.ORCID https://orcid.org/0000-0001-7394-9186
Qiang ZhangBeijing Key Laboratory of Complex Solid State Batteries, Department of Chemical Engineering, Tsinghua University, Beijing, P. R. China.

Funding

Beijing Municipal Natural Science Foundation L233004Beijing Municipal Natural Science Foundation L243019Beijing Municipal Natural Science Foundation L247015National Key Research and Development Program 2021YFB2500300National Natural Science Foundation of China 21825501National Natural Science Foundation of China 22308190National Natural Science Foundation of China 22393900National Natural Science Foundation of China 22393903National Natural Science Foundation of China 22509106National Natural Science Foundation of China 92472101National Natural Science Foundation of China T2322015
6 · The paper itself

Abstract

Hard carbon (HC) anode in sodium-ion batteries suffer from low initial Coulombic efficiency and irreversible capacity loss, limiting practical energy density and cycle life of SIBs. While direct-contact presodiation of HC has been proposed to increase the initial Coulombic efficiency of SIBs, but its low utilization efficiency can cause residual Na on the HC surface, resulting in rapid degradation and even safety concerns. Herein, we proposed a soft-contact presodiation (SCP) method, which can remove and recycle Na source and therefore greatly improve the utilization of the Na source and safety of SIBs. The SCP-treated HC anode achieves a ≈30.0% increase in ICE when paired with a NaNi

Indexed as

hard carbon anodehigh initial Coulombic efficiencysodium‐ion batteriessoft‐contact presodiationsolid electrolyte interphase

Identifiers

PMID42376776
PMCPMC13528560

What OpenQuestion holds

Textmetadata
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.