Evidence map›Paper›PMID 42257435›Full record

ArticleNano letters2026

Crack-Free Precision during Desiccation: Optimizing Aerosol Jet Printing for High-Performance Conductive Microstructure Manufacturing.

Geng Li, Yuxin Sun, Yanhong Tian, Jing Yu, Karol Viviana Mejia-Centeno, Malik Dilshad Khan, Shang Wang, Jordi Arbiol, Andreu Cabot, Qing Sun

Abstract read
In one paragraph

Article in Nano letters, 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

10 authors.

Geng LiState Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China.
Yuxin SunState Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China.
Yanhong TianState Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China.ORCID 0000-0002-5877-7096
Jing YuCatalonia Institute for Energy Research (IREC), Sant Adrià de Besòs, Barcelona 08930, Spain.
Karol Viviana Mejia-CentenoCatalonia Institute for Energy Research (IREC), Sant Adrià de Besòs, Barcelona 08930, Spain.
Malik Dilshad KhanCatalonia Institute for Energy Research (IREC), Sant Adrià de Besòs, Barcelona 08930, Spain.ORCID 0000-0002-3316-041X
Shang WangState Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China.
Jordi ArbiolCatalan Institute of Nanoscience and Nanotechnology (ICN2), CSIC and BIST, Campus UAB, Bellaterra, Barcelona 08193, Spain.ORCID 0000-0002-0695-1726
Andreu CabotCatalonia Institute for Energy Research (IREC), Sant Adrià de Besòs, Barcelona 08930, Spain.ORCID 0000-0002-7533-3251
Qing SunState Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China.ORCID 0000-0002-9145-7772

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Aerosol jet printing (AJP) is a high-resolution additive manufacturing technique that enables the deposition of conductive materials onto diverse substrates. However, a significant challenge in AJP is the occurrence of cracking in printed lines, which undermines both electrical conductivity and structural integrity. Herein, we examine the desiccation-induced cracking mechanism in AJP and introduce optimization strategies to mitigate cracking and enhance the conductivity of printed silver lines. Through a detailed analysis of crack morphology and distribution, key factors such as the deposition thickness and overspray regions are identified. The proposed optimizations, comprising regulation of the deposition thickness, enhancement of resolution, and minimization of overspray, yielded crack-free, high-quality silver lines with superior conductivity. These findings offer crucial insights for the advancement of reliable conductive structures in conformal electronics and microelectronics applications.

Indexed as

Additive manufacturingAerosol jet printingConductive microstructureDesiccation crackingSuction stress

Identifiers

PMID42257435
PMCPMC13281531

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.