Suppressing Surface Degradation in Na-Rich Prussian Blue Cathodes via Liquid-Phase Dehydration.

Seunghye Jang, Hyebin Jeong, Jun Choi, Jeongsoo Hong, Jooyoung Jang, Jongyoon Han, Juwon Kim, Sang-Min Lee, Changshin Jo

Abstract read
In one paragraph

Article in Advanced materials (Deerfield Beach, Fla.), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

9 authors.

Seunghye JangDepartment of Battery Engineering, Graduate Institute of Ferrous & Eco Materials Technology, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.ORCID https://orcid.org/0009-0005-4629-9380
Hyebin JeongDepartment of Chemical Engineering, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.
Jun ChoiDepartment of Battery Engineering, Graduate Institute of Ferrous & Eco Materials Technology, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.
Jeongsoo HongDepartment of Chemical Engineering, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.
Jooyoung JangDepartment of Battery Engineering, Graduate Institute of Ferrous & Eco Materials Technology, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.
Jongyoon HanResearch Institute of Industrial Science & Technology (RIST), Pohang, Gyeongbuk, Republic of Korea.
Juwon KimResearch Institute of Industrial Science & Technology (RIST), Pohang, Gyeongbuk, Republic of Korea.
Sang-Min LeeDepartment of Battery Engineering, Graduate Institute of Ferrous & Eco Materials Technology, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.ORCID https://orcid.org/0000-0002-3186-0447
Changshin JoDepartment of Battery Engineering, Graduate Institute of Ferrous & Eco Materials Technology, Pohang University of Science and Technology (POSTECH), Pohang, Gyeongbuk, Republic of Korea.ORCID https://orcid.org/0000-0002-2533-2197

Funding

Korea government (MOTIE) 20228510070100Korea Government (MOTIE) RS-2024- 00419413Korea Institute for Advancement of TechnologyKorea Institute of Energy Technology Evaluation and Planning (KETEP)Ministry of Trade, Industry & Energy(MOTIE, Korea) 2410000677Technology Innovation Program
6 · The paper itself

Abstract

Na-rich Prussian Blue (PB) is an attractive sodium-ion battery cathode owing to its high capacity and low cost, yet approximately 10 wt.% of crystal water in its framework induces electrolyte side reactions and Fe dissolution. Conventional thermal dehydration has been used to remove crystal water, but it consistently results in capacity fading and poor air stability. Here, the primary cause of degradation is experimentally demonstrated to be surface oxidation driven by Fe-O bond formation during heat treatment. Guided by this insight, a liquid-phase, low-temperature dehydration strategy based on nitrogen bubbling is introduced, which simultaneously eliminates crystal water and stabilizes the surface. The approach can be seamlessly integrated into electrode fabrication to minimize air exposure and improve cycling stability. Overall, this work clarifies the mechanistic role of surface oxidation in moisture-sensitive PB cathodes and highlights the critical importance of surface chemistry control in achieving stable electrochemical performance.

Indexed as

dehydrationmoisture stabilityprussian bluesodium‐ion batteriessurface oxidation

Identifiers

PMID42204870
PMCPMC13310102

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.