Evidence map›Paper›PMID 41774101›Full record

ArticleWorld journal of microbiology & biotechnology2026

Identification and evaluation of thermophilic bacteria isolated from Malaysian hot springs with potential for plastic polyvinyl chloride degradation.

Seng Chiew Toh, Sui Sien Leong, Samuel Lihan, Azizul Hakim Lahuri, Sabrina Rancang Khairul, Syeed Saifulazry Osman Al Edrus

Abstract read
In one paragraph

Article in World journal of microbiology & biotechnology, 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors.

Seng Chiew TohDepartment of Animal Sciences and Fishery, Faculty of Agricultural and Forestry Sciences, Universiti Putra Malaysia Sarawak, Bintulu, 97008, Malaysia.ORCID http://orcid.org/0000-0002-4279-5062
Sui Sien LeongDepartment of Animal Sciences and Fishery, Faculty of Agricultural and Forestry Sciences, Universiti Putra Malaysia Sarawak, Bintulu, 97008, Malaysia. leongsuisien@upm.edu.my.ORCID http://orcid.org/0000-0002-7050-2802
Samuel LihanInstitute of Biodiversity and Environmental Conservation, Universiti Malaysia Sarawak, Kota Samarahan, 94300, Malaysia.ORCID http://orcid.org/0000-0001-6791-4390
Azizul Hakim LahuriDepartment of Science and Technology, Faculty of Humanities, Management and Science, Universiti Putra Malaysia Sarawak, Bintulu, 97008, Malaysia.ORCID http://orcid.org/0000-0001-5057-3761
Sabrina Rancang KhairulInstitute of Ecosystem Science Borneo, Universiti Putra Malaysia Sarawak, Bintulu, 97008, Malaysia.ORCID http://orcid.org/0009-0008-8144-9761
Syeed Saifulazry Osman Al EdrusInstitute of Ecosystem Science Borneo, Universiti Putra Malaysia Sarawak, Bintulu, 97008, Malaysia.ORCID http://orcid.org/0000-0003-1093-0968

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

The biodegradation of polymeric plastics using biological agents has gained increasing interest. Thermophilic bacteria are particularly attractive as elevated temperatures weaken polymer structures, enhance substrate diffusion, and stimulate enzyme activity, thereby accelerating degradation. This study examined the thermophilic microbial degradation of polyvinyl chloride (PVC) by isolating, screening, and characterising effective PVC-degrading bacteria from three Malaysian hot springs. Sediment (50 g) and surface water (250 mL, 0–10 cm depth) were collected aseptically from three sites per hot spring. Physicochemical parameters (pH, temperature, salinity) were measured in triplicate. Samples were enriched in CFSM medium containing 0.1% (w/v) PVC powder and incubated at 55 °C for one week. Cultures were diluted and spread on carbon-free synthetic medium (CFSM) agar with PVC for viable counts. Isolates were screened using clear zone and bacterial adhesion to hydrocarbon (BATH) assays. Selected strains underwent 16 S rRNA sequencing, phylogenetic analysis, and RNA secondary structure prediction. Paku hot spring exhibited the highest bacterial density (5.49 ± 0.01 log₁₀ CFU/mL), highest pH (6.40 ± 0.22), and lowest temperature (37.87 ± 1.21 °C), classifying it as a thermal neutral spring. Panchor was a hyperthermal weak acid spring (pH 5.36 ± 0.07; 42.33 ± 1.01 °C), while Ayer Hangat was hyperthermal neutral with the highest salinity (28.20–28.37 ppt). From 288 isolates, 264 produced clearance zones (10–25 mm). Hydrophobicity analysis revealed 167 hydrophilic, 85 moderately hydrophobic, and 10 strongly hydrophobic isolates. Molecular identification confirmed Brevibacillus thermoruber (n = 1) and Anoxybacillus rupiensis (n = 9). In conclusion, the thermophilic bacterial isolates from three Malaysian hot springs demonstrated preliminary indications of PVC-interacting capability via clear zone formation and hydrophobicity. These isolates require further validation through quantitative degradation assays to reveal the PVC-degrading potential, underscoring their promise for plastic biodegradation and environmental remediation.

Indexed as

BacteriaHot SpringsPlasticsPolyvinyl ChlorideBacterial AdhesionBiodegradation, EnvironmentalDNA, BacterialGeologic SedimentsHot TemperatureHydrogen-Ion ConcentrationMalaysiaPhylogenyRNA, Ribosomal, 16STemperatureDNA, BacterialPlasticsPolyvinyl ChlorideRNA, Ribosomal, 16SBiodegradationHot springsMicrobialPolyvinyl chlorideThermophiles

Identifiers

PMID41774101
PMCPMC12957119

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.