Mechanical Property Evolution and Mechanisms of Polyolefins Under Thermo-Oxidative Aging.
Article in Polymers, 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
7 authors.
Funding
Abstract
Polyolefin materials are widely used due to their excellent properties and low cost. However, in high-temperature oxygen environments, they are susceptible to thermo-oxidative aging, which reduces mechanical properties and durability. This study systematically analyzed the aging behavior and mechanisms of polyolefins at varying temperatures and exposure durations through accelerated thermal oxidation experiments. The results indicate that the thermo-oxidative aging behavior of polyolefins can be divided into three stages. In Stage I, elevated temperature promotes segmental mobility and chain rearrangement, which increases crystallinity and temporarily improves mechanical properties. In Stage II, antioxidants are progressively consumed and oxygen-containing groups begin to accumulate, resulting in reduced crystallinity, a decline in mechanical performance, and the onset of slight surface yellowing. In Stage III, the antioxidant system is largely depleted and oxidative reactions are intensified, leading to mainchain scission and molecular weight reduction. This causes a further decrease in crystallinity, a significant deterioration in both strength and toughness, accompanied by aggravated yellowing. This study elucidates the thermo-oxidative aging mechanism of polyolefins, providing a theoretical basis for assessing their service life and evaluating the stability of waste plastics.