ArticleChemistry of materials : a publication of the American Chemical Society2025
Effect of Annealing on Direct Recycled NMC Cathodes.
Article in Chemistry of materials : a publication of the American Chemical Society, 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
- Recycling nickel-rich cathodes toward structural and functional circularity: a perspective.Chemical science · 2026Review
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
15 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
A substantial number of electric vehicle batteries are poised to reach end-of-life conditions in the next decade. Direct recycling has advantages over typical recycling processes because it preserves the chemical structure of the material. One key step of direct recycling materials like nickel manganese cobalt oxide (NMC) cathodes is relithiation, which includes replacing the depleted lithium inventory in the cathode and annealing the material to fix crystallographic degradation. This work uses multiple characterization techniques (synchrotron X-ray diffraction, Ni X-ray absorption near edge structure, scanning transmission electron microscopy) to understand the lithiation mechanism of degraded and chemically relithiated NMC 622. Despite the necessary reconstruction after relithiation being limited to the surface of the degraded NMC 622, a high annealing temperature of 720 °C is still necessary to restore the NMC 622 structure back to pristine condition after relithiation. This work also finds that treating degraded NMC 622 with an annealing step is sufficient to restore key electrochemical and structural properties, other essential features of pristine NMC 622 material such as particle porosity and morphology are largely unaffected. Understanding the effect of this annealing step has important implications on defining the degree of success of any given direct recycling strategy.