Evidence map›Paper›PMID 41598095›Full record

ArticleMaterials (Basel, Switzerland)2026

Degradation of Some Polymeric Materials of Bioreactors for Growing Algae.

Ewa Borucińska-Parfieniuk, Ewa Górecka, Jakub Markiewicz, Urszula Błaszczak, Krzysztof J Kurzydlowski, Izabela B Zglobicka

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2026. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors.

Ewa Borucińska-ParfieniukFaculty of Mechanical Engineering, Bialystok University of Technology, 45C Wiejska Str., 15-351 Bialystok, Poland.ORCID 0009-0004-2376-4078
Ewa GóreckaInstytut Nauk o Morzu i Środowisku, Uniwersytet Szczeciński, 16A Mickiewicza Str., 70-383 Szczecin, Poland.ORCID 0000-0003-0590-7480
Jakub MarkiewiczFaculty of Electrical Engineering, Bialystok University of Technology, 45C Wiejska Str., 15-351 Bialystok, Poland.ORCID 0000-0002-9763-4602
Urszula BłaszczakFaculty of Electrical Engineering, Bialystok University of Technology, 45C Wiejska Str., 15-351 Bialystok, Poland.ORCID 0000-0003-1967-0365
Krzysztof J KurzydlowskiFaculty of Mechanical Engineering, Bialystok University of Technology, 45C Wiejska Str., 15-351 Bialystok, Poland.ORCID 0000-0003-3875-4820
Izabela B ZglobickaFaculty of Mechanical Engineering, Bialystok University of Technology, 45C Wiejska Str., 15-351 Bialystok, Poland.ORCID 0000-0002-4432-9196

Funding

Bialystok University of Technology WZ/WM-IIM/3/2023Ministry of Science and Higher Education RID/SP/0026/2024/01
6 · The paper itself

Abstract

Transparent polymeric materials such as poly(methyl methacrylate) (PMMA), polycarbonate (PC), and polyethylene terephthalate (PET) are widely used as glass alternatives in algal bioreactors, where optical clarity and mechanical stability are crucial. However, their long-term use is limited by surface degradation processes. Photodegradation, hydrolysis, and biofilm accumulation can reduce light transmission in the 400-700 nm range essential for photosynthesis. This study examined the aging of PMMA, PC, and PET under bioreactor conditions. Samples were exposed for 70 days to illumination, culture medium, and aquatic environments. Changes in their optical transmittance, surface roughness, and wettability were analyzed. All polymers exhibited measurable surface degradation, characterized by an average 15% loss in transparency, significant increases in surface roughness, and reduced contact angles. PMMA demonstrated the highest optical stability, maintaining strong transmission in key blue and red spectral regions, while PET performed the worst, showing low initial clarity and the steepest decline. The most severe surface degradation occurred in areas exposed to the receding liquid interface, highlighting the need for targeted cleaning and/or a reduction in the size of the liquid-vapor transition zone. Overall, the results identify PMMA and recycled PMMA (PMMA

Indexed as

algal bioreactorsbioreactorsoptical transmittancephotodegradationtransparent polymers

Identifiers

PMID41598095
PMCPMC12842760

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.