Morphology of Fumes from Hybrid Laser-Arc Welding of X5CrNi18-10 Stainless Steel.

Janusz Adamiec, Joanna Wyciślik-Sośnierz, Jolanta Matusiak, Michał Urbańczyk, Marcin Lemanowicz, Robert Kusiorowski, Anna Gerle

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.

0numbers the graph read from it
0cells of the map it votes in
1citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

1 citing paper in PubMed.

  1. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

7 authors.

Janusz AdamiecFaculty of Materials Engineering and Digitalisation of Industry, Silesian University of Technology, 40-019 Katowice, Poland.ORCID 0000-0002-9135-6138
Joanna Wyciślik-SośnierzŁukasiewicz Research Network-Upper Silesian Institute of Technology, 44-100 Gliwice, Poland.
Jolanta MatusiakŁukasiewicz Research Network-Upper Silesian Institute of Technology, 44-100 Gliwice, Poland.ORCID 0000-0002-2134-027X
Michał UrbańczykŁukasiewicz Research Network-Upper Silesian Institute of Technology, 44-100 Gliwice, Poland.ORCID 0000-0001-8015-3338
Marcin LemanowiczFaculty of Chemistry, Silesian University of Technology, 44-100 Gliwice, Poland.ORCID 0000-0002-1679-6221
Robert KusiorowskiŁukasiewicz Research Network-Institute of Ceramics and Building Materials, 31-983 Cracow, Poland.ORCID 0000-0002-5594-774X
Anna GerleŁukasiewicz Research Network-Institute of Ceramics and Building Materials, 31-983 Cracow, Poland.ORCID 0000-0002-1223-3683

Funding

Silesian University of Technology 11/020/RGJ25/0141
6 · The paper itself

Abstract

Stainless steels are widely used across many industrial sectors, including the fabrication of welded structures. The most common methods for joining these materials are arc welding processes. Increasing demands for higher weld quality and process efficiency have led to a growing adoption of laser-based technologies in industry. One of the most frequently applied techniques is hybrid laser-arc welding (HLAW), which combines two heat sources-the laser beam and the electric arc-acting simultaneously. For new, innovative joining technologies, a critical factor in their implementation is their impact on the environment and human health. This article presents the results of a study on the morphology of fumes emitted during the HLAW of X5CrNi18-10 (1.4301) stainless steel. Laser diffraction and scanning electron microscopy were used to characterize the fume morphology. The International Agency for Research on Cancer has classified welding fumes as a carcinogenic agent to humans. The results revealed that more than 20% of particles generated during hybrid welding belong to the most hazardous fraction, as they can penetrate beyond the laryngeal region. These particles exhibit a homogeneous elemental distribution, with the chromium content standing at approximately 20% and nickel nearly 10%.

Indexed as

hybrid weldinglaser diffractionmorphologySEM-EDS (Scanning Electron Microscopy with Energy Dispersive Spectroscopy)stainless steelwelding fume

Identifiers

PMID41470306
PMCPMC12735081

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.