ArticleBMC oral health2025

Effect of multiple firings on mechanical and optical properties of CAD/CAM lithium disilicate-based glass ceramics.

Chawal Padunglappisit, Pitsucha Charoensakthanakul, Sintwo Wongthongdee, Kan Wongkamhaeng

Abstract read
In one paragraph

Article in BMC oral health, 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors.

Chawal PadunglappisitDivision of Prosthodontics, Faculty of Dentistry, Thammasat University, 99 M 18 Paholyothin Road, Klong Nueng, Klong Laung, Pathumthani, 12121, Thailand.
Pitsucha CharoensakthanakulDivision of Prosthodontics, Faculty of Dentistry, Thammasat University, 99 M 18 Paholyothin Road, Klong Nueng, Klong Laung, Pathumthani, 12121, Thailand.
Sintwo WongthongdeeDivision of Prosthodontics, Faculty of Dentistry, Thammasat University, 99 M 18 Paholyothin Road, Klong Nueng, Klong Laung, Pathumthani, 12121, Thailand.
Kan WongkamhaengDivision of Prosthodontics, Faculty of Dentistry, Thammasat University, 99 M 18 Paholyothin Road, Klong Nueng, Klong Laung, Pathumthani, 12121, Thailand. kw_dent@tu.ac.th.

Funding

Thammasat University Research Grants No. 9/2566
6 · The paper itself

Abstract

purposeThe longevity of computer-aided design and computer-aided manufacturing (CAD/CAM) lithium disilicate-based restoration varies significantly depending on the type of restoration, the properties of materials used, and their esthetics. This study investigated the effect of multiple firings on flexural strength, microhardness, bond strength, and color stability of different CAD/CAM lithium disilicate-based glass ceramics. MATERIALS AND

methodsThree different lithium disilicate-based glass ceramics, IPS e.max CAD (EM), CEREC Tessera (CT), and LiSi CAD (LC) were wet-sectioned into rectangular (approximately 14.5 × 12.4 × 1.2 mm

resultsAccording to the 2-way ANOVA, the color stability was significantly influenced by both materials and number of firing cycles. The color stability of LC statistically significant increased upon increasing the number of firings (p < 0.0001). In addition, a significant between materials and number of firings was also observed (p < 0.0001). There was no apparent impact on the biaxial flexural strength and microhardness from multiple firings (p > 0.05). However, EM exhibited the highest biaxial flexural strength, while LC showed the highest microhardness, regarding to the materials (p < 0.0001). For shear bond strength, material (p < 0.001) and number of firings (p = 0.0277) were found significant, specifically LiSi CAD.

conclusionThere was no apparent impact on biaxial flexural strength and microhardness of CAD/CAM lithium disilicate-based glass ceramics after multiple firings. However, multiple firings affected the color stability and shear bond strength of lithium disilicate-based glass ceramics. The color change was noticeable after the third firing cycle, specifically CEREC Tessera. The shear bond strength of LiSi CAD increased as a function of multiple firings. Cautiously corrective adjustments and recontouring are required to minimize the unessential firings.

Indexed as

CeramicsComputer-Aided DesignDental PorcelainColorDental BondingDental Prosthesis DesignDental Stress AnalysisFlexural StrengthHardnessHumansMaterials TestingSurface PropertiesDental PorcelainGlass ceramicslithia disilicateAdvanced lithium disilicateBiaxial flexural strengthColor stabilityLithium disilicateMicrohardnessShear bond strength

Identifiers

PMID41275144
PMCPMC12751732

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.