Evidence map›Paper›PMID 41156953›Full record

ArticleMaterials (Basel, Switzerland)2025

A Method for Identifying Hydration Stages of Concrete Based on Embedded Piezo-Ultrasonic Active Sensing Technology.

Min Xiao, Yaoting Zhu, Wei Min, Feilong Ye, Yongwei Li, Xunhao Ding, Tao Ma

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.

0numbers the graph read from it
0cells of the map it votes in
1citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

1 citing paper in PubMed.

  1. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

7 authors.

Min XiaoJiangxi Communications Investment Group Co., Ltd., No. 367, Chaoyangzhou Middle Road, Nanchang 330025, China.
Yaoting ZhuJiangxi Communications Investment Maintenance Technology Group, No. 809, Jinsan Avenue, Xiaolan Economic Development Zone, Nanchang 330052, China.
Wei MinJiangxi Communications Investment Group Co., Ltd., No. 367, Chaoyangzhou Middle Road, Nanchang 330025, China.
Feilong YeSchool of Transportation, Southeast University, Nanjing 211186, China.
Yongwei LiJiangxi Communications Investment Group Co., Ltd., No. 367, Chaoyangzhou Middle Road, Nanchang 330025, China.
Xunhao DingSchool of Transportation, Southeast University, Nanjing 211186, China.
Tao MaSchool of Transportation, Southeast University, Nanjing 211186, China.ORCID 0000-0002-7963-9370

Funding

Xunhao Ding BK20220844Xunhao Ding HEKLSP2022-02Xunhao Ding JSSCBS20220094Xunhao Ding NO.52208427Xunhao Ding NO.52378445Xunhao Ding TAM202201
6 · The paper itself

Abstract

The structural evolution of concrete during different hydration stages critically influences subsequent strength, and continuous monitoring throughout this process has become a research focus in materials science. This study proposes an embedded ultrasonic active sensing technique based on piezoelectric ceramics (PZT) to identify key structural transition stages during concrete curing. To this end, a piezoelectric ultrasonic sensor was fabricated and its comprehensive performance was systematically evaluated. Subsequently, compressive strength and penetration resistance tests were conducted, and the evolution of piezoelectric signal amplitude and wavelet packet energy (WPE) during hydration was analyzed. Furthermore, a root mean square deviation index based on WPE (WPE-RMSD) was introduced to identify structural transitions throughout the hydration process. The results demonstrate that the developed sensor exhibits stable electrical, mechanical, and waterproof performance. Both signal amplitude and WPE effectively captured the hydration process of concrete, with WPE showing higher sensitivity. The WPE-RMSD index exhibited good temporal continuity, covering the entire process from early hydration disturbance to late-stage structural densification (28 d), and proved particularly effective in identifying critical stages such as final setting and the medium-age period (7 d). This study provides a novel in situ monitoring approach for the classification and identification of hydration stages in concrete.

Indexed as

compressive strengthconcrete hydrationpenetration resistancepiezoelectric sensingpiezoelectric wave propagation method (PWPM)setting time

Identifiers

PMID41156953
PMCPMC12566301

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.