ArticleMaterials (Basel, Switzerland)2025
Polar Cryogenic Impact Behavior of Selective Laser Melted Ti-6Al-4V Alloy: Effects of Scanning Strategies and Notch Orientation.
Article in Materials (Basel, Switzerland), 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
- 3D & 4D Printing-In Engineering Applications.Materials (Basel, Switzerland) · 2026Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
7 authors.
Funding
Abstract
The anisotropic mechanical properties of selective laser melting (SLM)-processed Ti-6Al-4V (TC4) alloy hinder its deployment in polar marine equipment. This study systematically probes the relationships between laser scanning strategies (unidirectional vs. 67°-rotated scanning between layers), notch orientation (governing loading direction), and cryogenic impact energy of SLM-TC4. Charpy impact tests from -60 °C to 20 °C were performed on V-notched specimens fabricated with distinct scanning strategies and notch orientations (top/side surfaces). The analysis of impact energy data and macro/micro-fractography demonstrates that impact energy declines markedly with decreasing temperature, showing a 25-35% reduction at -60 °C versus 20 °C while exhibiting enhanced data consistency under cryogenic conditions. Notably, specimens fabricated with 67°-rotated scanning between layers achieve higher impact toughness than unidirectionally scanned equivalents. Moreover, for identical scanning strategies, side-notched specimens consistently outperform top-notched specimens, evidencing superior interfacial bonding strength between deposited layers relative to bonding within individual layers. Within individual layers, toughness normal to the laser scan path exceeds that parallel to the path. However, controlling ductile-to-brittle transition behavior and precluding brittle failure are imperative for SLM-TC4 components in polar cryogenic service. This work delivers essential quantitative benchmarks and experimental validation for optimizing SLM processing in critical polar vessel components.