Evidence map›Paper›PMID 40720161›Full record

ArticleAdvanced science (Weinheim, Baden-Wurttemberg, Germany)2025

Molecular Damping Effect of Trace Additives Enhances Zinc Anode Stability Under High Depth of Discharge.

Yue Li, Hao Xu, Xiaodong Li, Xi Lin, Hongyang Zhao, Yajuan Zhang, Kwun Nam Hui, Jinliang Li, Likun Pan

Abstract read
In one paragraph

Article in Advanced science (Weinheim, Baden-Wurttemberg, Germany), 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed.

  1. Article
  2. Review
  3. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

9 authors.

Yue LiShanghai Key Laboratory of Magnetic Resonance, School of Physics and Electronic Science, Institute of Magnetic Resonance and Molecular Imaging in Medicine, East China Normal University, Shanghai, 200241, P. R. China.
Hao XuFaculty of Chemistry and Food Chemistry and Center for Advancing Electronics Dresden, Technische Universität Dresden, 01062, Dresden, Germany.
Xiaodong LiFaculty of Chemistry and Food Chemistry and Center for Advancing Electronics Dresden, Technische Universität Dresden, 01062, Dresden, Germany.
Xi LinShanghai Key Laboratory of Hydrogen Science and Center of Hydrogen Science, Shanghai Jiao Tong University, Shanghai, 200240, P. R. China.
Hongyang ZhaoShanghai Key Laboratory of Magnetic Resonance, School of Physics and Electronic Science, Institute of Magnetic Resonance and Molecular Imaging in Medicine, East China Normal University, Shanghai, 200241, P. R. China.
Yajuan ZhangSchool of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai, 200240, P. R. China.
Kwun Nam HuiJoint Key Laboratory of the Ministry of Education, Institute of Applied Physics and Materials Engineering, University of Macau, Avenida da Universidade, Taipa, Macau SAR, 519000, P. R. China.
Jinliang LiSiyuan Laboratory, Guangdong Provincial Engineering Technology Research Center of Vacuum Coating Technologies and New Energy Materials, Department of Physics, College of Physics & Optoelectronic Engineering, Jinan University, Guangzhou, 510632, P. R. China.
Likun PanShanghai Key Laboratory of Magnetic Resonance, School of Physics and Electronic Science, Institute of Magnetic Resonance and Molecular Imaging in Medicine, East China Normal University, Shanghai, 200241, P. R. China.ORCID https://orcid.org/0000-0001-9294-1972

Funding

China Scholarship CouncilFundamental Research Funds for the Central Universities YBNLTS2025-024Guangxi Science and Technology Program 2024AB08156International Partnership Program of Chinese Academy of Sciences 124GJHZ2023031MIMinistry of Science and Technology of China G2023199002L
6 · The paper itself

Abstract

Resolving the severe issues such as electric field distortion, dendritic zinc growth, and uneven zinc deposition under high depths of discharge (DOD) has become a significant hurdle of the aqueous zinc-ion batteries (ZIBs). To address these challenges, an interfacial regulation strategy is proposed based on the molecular damping effect, in which a trace amount of weakly adsorbing additive is employed to stabilize the Zn anode interface by mitigating energy shocks and ionic disturbances induced by electric field fluctuations. Trace perfluorinated PSVE (erfluoro-3,6-dioxa-4-methyloct-7-enesulphonyl fluoride) is introduced to the traditional ZnSO

Indexed as

aqueous zinc‐ion batterieshigh depth of dischargemolecular damping effectPSVEtrace additive

Identifiers

PMID40720161
PMCPMC12499422

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.