ArticleBMC oral health2025
Impact of deglazing on biaxial flexural strength of high translucent zirconia: effect of hydrothermal aging, pH-cycling, and load-cycling.
Article in BMC oral health, 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
3 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
backgroundTo compare the effect of deglazing and aging on biaxial flexural strength (FS) of high translucent (HT) zirconia.
methods40 disc-shaped specimens (12 × 1.2 mm) of HT zirconia (3Y-PSZ, Upcera HT) were sintered after milling, glazed(G) and randomly assigned equally into 4 experimental groups: G) glazing; G-A) glazing, aging; DG-A) deglazing, aging; and NG-A) non-glazing, aging. A sequence of three methods was used for aging; hydrothermal, pH-cycling, and load cycling. FS(flexural strength) of all specimens was measured and one specimen from each group underwent X-ray diffraction (XRD) for assessment of phase transformation (t-m). Distribution of data was evaluated using the Kolmogorov -Smirnov test, and with respect to the confidence interval of 95%, data were analyzed using 1-way ANOVA with statistical software (IBM SPSS Statisticsv20.0) to compare the mean flexural strength values among the 4 groups. When significant differences were found, the mean values were compared using Tukey's honest significant difference (HSD) test (α = 0.05).
resultsFS of glazed specimens (1092.78 ± 175.40 MPa
conclusionLoss of glaze layer and no glazing had no significant effect on FS of high translucent Y-PSZ after aging.