Quantitative characterization of indentation initiated crack growth in bovine enamel.

Heng Xiao, Lei Lei, Jing Zheng, Zhongrong Zhou

Abstract read
In one paragraph

Article in Scientific reports, 2025. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers, 1 of them a synthesis that pooled it.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed, 1 pooled it
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed, 1 synthesis or guideline pooled it.

  1. Pooled it
  2. Article
  3. Review
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors.

Heng XiaoSchool of Mechanical Engineering, Xihua University, Chengdu, 610039, China.
Lei LeiTribology Research Institute, Key Laboratory of Advanced Technologies of Materials, Ministry of Education, Southwest Jiaotong University, Chengdu, 610031, China.
Jing ZhengTribology Research Institute, Key Laboratory of Advanced Technologies of Materials, Ministry of Education, Southwest Jiaotong University, Chengdu, 610031, China. jzheng168@home.swjtu.edu.cn.
Zhongrong ZhouTribology Research Institute, Key Laboratory of Advanced Technologies of Materials, Ministry of Education, Southwest Jiaotong University, Chengdu, 610031, China.

Funding

111 Project B20008National Natural Science Foundation of China 52075459Sichuan Science and Technology Program 2023NSFSC0867
6 · The paper itself

Abstract

In this in vitro study, indentation cracks in orthogonal directions and different areas on bovine enamel occlusal surface were analyzed by quantitative characterization of crack number, length and displacement, aiming to reveal the correlation between the microstructure and crack growth behavior of bovine enamel. Results showed that the cracks induced by indenting on the enamel occlusal surface tend to initiate at the rod/inter-rod boundaries. The rod/inter-rod hydroxyapatite (HAP) nanofibers and associated decussation cause a preferential extension of the cracks along the rod/inter-rod interface by inducing crack deflection, bifurcation, and bridging. In addition, the inter-rod nano-structure, consisting of orderly assembled HAP nanofibers, leads to an additional toughening mechanism of zig-zag cracking to hinder crack growth within the narrow inter-rod region. In summary, the unique microstructural architecture of bovine enamel, especially the decussation within rod/inter-rod nanofibers, plays an important role in functionally guiding cracks on bovine enamel occlusal surface to grow along the interface between rod and inter-rod rather than across the inter-rod enamel. The anisotropic crack growth behavior helps prevent bovine enamel from substantial fracture and chipping induced wear. These findings extend the understanding of the toughening mechanisms of mammalian enamel.

Indexed as

Dental EnamelTooth FracturesAnimalsCattleDurapatiteNanofibersSurface PropertiesDurapatiteAnisotropyBovine enamelCrack growthIndentation crackNanofiber

Identifiers

PMID40108352
PMCPMC11923090

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.