Evidence map›Paper›PMID 39339455›Full record

ArticleMolecules (Basel, Switzerland)2024

Modulation of Free Carbon Structures in Polysiloxane-Derived Ceramics for Anode Materials in Lithium-Ion Batteries.

Yiling Quan, Changhao Hu, Peifeng Feng, Yujie Song, Kun Liang, Xigao Jian, Jian Xu

Abstract read
In one paragraph

Article in Molecules (Basel, Switzerland), 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

7 authors.

Yiling QuanState Key Laboratory of Fine Chemicals, Liaoning High Performance Polymer Engineering Research Center, Department of Polymer Science and Materials, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.
Changhao HuState Key Laboratory of Fine Chemicals, Liaoning High Performance Polymer Engineering Research Center, Department of Polymer Science and Materials, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.
Peifeng FengState Key Laboratory of Fine Chemicals, Liaoning High Performance Polymer Engineering Research Center, Department of Polymer Science and Materials, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.
Yujie SongZhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China.ORCID 0000-0001-9600-8530
Kun LiangZhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China.ORCID 0000-0001-5551-1439
Xigao JianState Key Laboratory of Fine Chemicals, Liaoning High Performance Polymer Engineering Research Center, Department of Polymer Science and Materials, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.
Jian XuState Key Laboratory of Fine Chemicals, Liaoning High Performance Polymer Engineering Research Center, Department of Polymer Science and Materials, School of Chemical Engineering, Dalian University of Technology, Dalian 116024, China.

Funding

Fundamental Research Funds for the Central Universities DUT22-LAB605National Natural Science Foundation of China 52075526National Natural Science Foundation of China 91860204Ningbo 3315 Plan Innovation Team 2017A-28-C
6 · The paper itself

Abstract

Polymer-derived silicon oxycarbide (SiOC) ceramics have garnered significant attention as novel silicon-based anode materials. However, the low conductivity of SiOC ceramics is a limiting factor, reducing both their rate capability and cycling stability. Therefore, controlling the free carbon content and its degree of graphitization within SiOC is crucial for determining battery performance. In this study, we regulated the free carbon content using divinylbenzene (DVB) and controlled the graphitization of free carbon with the transition metal iron (Fe). Through a simple pyrolysis process, we synthesized SiOC ceramic materials (CF) and investigated the impact of Fe-induced changes in the carbon phase and the amorphous SiOC phase on the comprehensive electrochemical performance. The results demonstrated that increasing the DVB content in the SiOC precursor enhanced the free carbon content, while the addition of Fe promoted the graphitization of free carbon and induced the formation of carbon nanotubes (CNTs). The electrochemical performance results showed that the CF electrode material exhibited a high reversible capacity of approximately 1154.05 mAh g

Indexed as

carbon nanotubesfree carbonpolymer-derived ceramicsSiOC anode

Identifiers

PMID39339455
PMCPMC11434428

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.