Long-Term Bonding Performance of One-Bottle vs. Two-Bottle Bonding Agents to Lithium Disilicate Ceramics.
Article in Polymers, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
3 citing papers in PubMed.
- Article
- Does simplification signify compromise? Evaluation of different universal adhesives on shear bond strength:Frontiers in bioengineering and biotechnology · 2026Article
- Bond Strength of Universal Adhesive/Resin Cement Combinations Relying on Touch-Cure Mechanisms.Polymers · 2025Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
5 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The aim of this study was to compare the long-term bonding performance to lithium disilicate (LDS) ceramic between one-bottle and two-bottle bonding agents. Bonding performance was investigated under these LDS pretreatment conditions: with hydrofluoric acid (HF) only, without HF, with a two-bottle bonding agent (Tokuyama Universal Bond II) only. Shear bond strengths between LDS and nine resin cements (both self-adhesive and conventional adhesive types) were measured at three time periods: after one-day water storage (Base), and after 5000 and 20,000 thermocycles (TC 5k and TC 20k respectively). Difference in degradation between one- and two-bottle bonding agents containing the silane coupling agent was compared by high-performance liquid chromatography. With HF pretreatment, bond strengths were not significantly different among the three time periods for each resin cement. Without HF, ESTECEM II and Super-Bond Universal showed significantly higher values than others at TC 5k and TC 20k when treated with the recommended bonding agents, especially at TC 20k. Difference in degradation between one- and two-bottle bonding agents containing the silane coupling agent was compared by high-performance liquid chromatography (HPLC). For both cements, these values at TC 20k were also not significantly different from pretreatment with only Tokuyama Universal Bond II. For LDS, long-term bond durability could be maintained by pretreatment with Tokuyama Universal Bond II instead of the hazardous HF.