ArticleBioactive materials2024
High-performance Mg-Zn alloy achieved by the ultrafine grain and nanoparticle design.
Article in Bioactive materials, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
- Spatiotemporal Evolution of Interfacial pH and HMolecules (Basel, Switzerland) · 2026Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
10 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
Improving the comprehensive performance of low alloyed Mg is a significant challenge for biomedical applications. This paper developed a high-performance Mg-Zn alloy with uniform ultrafine grains and nano-precipitates through a straightforward, high-temperature reciprocating equal channel angle extrusion (ECAP) process and researched the microstructure, mechanical property, degradation behaviour, and biocompatibility of the developed alloy. Results showed that the lean Mg-2Zn alloy successfully refined grain to about 1 μm and produced plenty of nano-particles with uniform distribution, providing high comprehensive mechanical properties (YS: 235 MPa, UTS: 267 MPa, EL: 15.6 %). Additionally, Zn-riched nano-particles in the matrix could decrease the Zn aggregation at the corrosion layer-matrix interface and form a dense oxide film, achieving a low degradation rate (0.13 mm/year