Chemical Prelithiated 3D Lithiophilic/-Phobic Interlayer Enables Long-Term Li Plating/Stripping.

Sandro Schöner, Dana Schmidt, Xinchang Chen, Krzysztof Dzieciol, Roland Schierholz, Pengfei Cao, Ahmad Ghamlouche, Fabian Jeschull, Anna Windmüller, Chih-Long Tsai and 7 more

Abstract read
In one paragraph

Article in ACS nano, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 2 papers.

0numbers the graph read from it
0cells of the map it votes in
2citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

2 citing papers in PubMed.

  1. Article
  2. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

17 authors.

Sandro SchönerInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0001-6591-9462
Dana SchmidtInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0002-0827-1265
Xinchang ChenLaboratory of Advanced Spectro-electrochemistry and Li-Ion Batteries, Dalian Institute of Chemical Physics, Chinese Academy of Sciences, Dalian 116023, China.
Krzysztof DzieciolInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.
Roland SchierholzInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0002-2298-4405
Pengfei CaoErnst Ruska-Centre for Microscopy and Spectroscopy with Electrons, Forschungszentrum Jülich, 52428 Jülich, Germany.
Ahmad GhamloucheKarlsruher Institute of Technologie (KIT), Institute for Applied Materials-Energy Storage Systems (IAM-ESS), 76344 Eggenstein Leopoldshafen, Germany.
Fabian JeschullKarlsruher Institute of Technologie (KIT), Institute for Applied Materials-Energy Storage Systems (IAM-ESS), 76344 Eggenstein Leopoldshafen, Germany.ORCID 0000-0002-5927-1978
Anna WindmüllerInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0003-2829-3362
Chih-Long TsaiInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0001-8103-3514
Xunfan LiaoNational Engineering Research Center for Carbohydrate Synthesis/Key Lab of Fluorine and Silicon for Energy Materials and Chemistry of Ministry of Education, Jiangxi Normal University, 330022 Nanchang, China.ORCID 0000-0002-6649-5865
Hans KunglInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.
Gui-Ming ZhongLaboratory of Advanced Spectro-electrochemistry and Li-Ion Batteries, Dalian Institute of Chemical Physics, Chinese Academy of Sciences, Dalian 116023, China.ORCID 0000-0003-2313-4741
Yiwang ChenNational Engineering Research Center for Carbohydrate Synthesis/Key Lab of Fluorine and Silicon for Energy Materials and Chemistry of Ministry of Education, Jiangxi Normal University, 330022 Nanchang, China.ORCID 0000-0003-4709-7623
Hermann TempelInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0002-9794-6403
Shicheng YuInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0002-6619-3330
Rüdiger-A EichelInstitute of Energy and Climate Research (IEK-9: Fundamental Electrochemistry), Forschungszentrum Jülich, 52428 Jülich, Germany.ORCID 0000-0002-0013-6325

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

The up-to-date lifespan of zero-excess lithium (Li) metal batteries is limited to a few dozen cycles due to irreversible Li-ion loss caused by interfacial reactions during cycling. Herein, a chemical prelithiated composite interlayer, made of lithiophilic silver (Ag) and lithiophobic copper (Cu) in a 3D porous carbon fiber matrix, is applied on a planar Cu current collector to regulate Li plating and stripping and prevent undesired reactions. The Li-rich surface coating of lithium oxide (Li

Indexed as

anode-freeanode-lesscarbon fiberslithiophilic−lithiophobic gradientprelithiationzero-excess Li metal batteries

Identifiers

PMID38937963
PMCPMC11238590

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.