ArticlePolymers2024
Mechanochemical Recycling of Flexible Polyurethane Foam Scraps for Quantitative Replacement of Polyol Using Wedge-Block-Reinforced Extruder.
Article in Polymers, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
12 authors.
Funding
Abstract
Recycling flexible polyurethane foam (F-PUF) scraps is difficult due to the material's high cross-linking structure. In this work, a wedge-block-reinforced extruder with a considerable enhanced shear extrusion and stretching area between the rotating screw and the stationary wedge blocks was utilized to recycle F-PUF scraps into powder containing surface-active hydroxyl groups. The powder was then utilized for the quantitative replacement of polyol in the foaming process. Characterizations showed that the continuous shear extrusion and stretching during the extrusion process reduced the volume mean diameter (VMD) of the F-PUF powder obtained by extruding it three times at room temperature to reach 54 μm. The -OH number (OHN) of the powder prepared by extruding it three times reached 19.51 mgKOH/g due to the mechanochemical effect of the powdering method. The F-PUF containing recycled powder used to quantitively replace 10 wt.% polyol was similar in microstructure and chemical structure to the original F-PUF, with a compression set of 2%, indentation load deflection of 21.3 lbf, resilience of 43.4%, air permeability of 815.7 L/m
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.