Evidence map›Paper›PMID 38894026›Full record

ArticleMaterials (Basel, Switzerland)2024

Long-Term Thermal Stabilization of Poly(Lactic Acid).

Jannik Hallstein, Elke Metzsch-Zilligen, Rudolf Pfaendner

Abstract read
In one paragraph

Article in Materials (Basel, Switzerland), 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 5 papers.

0numbers the graph read from it
0cells of the map it votes in
5citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

5 citing papers in PubMed.

  1. Review
  2. Article
  3. Review
  4. Article
  5. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

3 authors.

Jannik HallsteinDivision Plastics, Fraunhofer Institute for Structural Durability and System Reliability LBF, 64289 Darmstadt, Germany.
Elke Metzsch-ZilligenDivision Plastics, Fraunhofer Institute for Structural Durability and System Reliability LBF, 64289 Darmstadt, Germany.
Rudolf PfaendnerDivision Plastics, Fraunhofer Institute for Structural Durability and System Reliability LBF, 64289 Darmstadt, Germany.

Funding

Fraunhofer-Gesellschaft e.V. Cluster of Excellence Circular Plastics Economy
6 · The paper itself

Abstract

To use polylactic acid in demanding technical applications, sufficient long-term thermal stability is required. In this work, the thermal aging of polylactic acid (PLA) in the solid phase at 100 °C and 150 °C is investigated. PLA has only limited aging stability without the addition of stabilizers. Therefore, the degradation mechanism in thermal aging was subsequently investigated in more detail to identify a suitable stabilization strategy. Investigations using nuclear magnetic resonance spectroscopy showed that, contrary to expectations, even under thermal aging conditions, hydrolytic degradation rather than oxidative degradation is the primary degradation mechanism. This was further confirmed by the investigation of suitable stabilizers. While the addition of phenols, phosphites and thioethers as antioxidants leads only to a limited improvement in aging stability, the addition of an additive composition to provide hydrolytic stabilization results in extended durability. Efficient compositions consist of an aziridine-based hydrolysis inhibitor and a hydrotalcite co-stabilizer. At an aging temperature of 100 °C, the time until significant polymer chain degradation occurs is extended from approx. 500 h for unstabilized polylactic acid to over 2000 h for stabilized polylactic acid.

Indexed as

antioxidantsdegradation mechanismshydrolysis stabilizerpoly(lactic acid)thermal aging

Identifiers

PMID38894026
PMCPMC11173481

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.