ArticleMaterials (Basel, Switzerland)2024
Corrosion Activity of Ultrafine-Grained Pure Magnesium and ZK60 Magnesium Alloy in Phosphate Buffered Saline Solution.
Article in Materials (Basel, Switzerland), 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
4 authors.
Funding
Abstract
The magnesium alloy ZK60 is a promising candidate as a material for biodegradable implants. One of the most important factors for biodegradable implants is the modification of their corrosion behavior to match the requirements for the healing bone or tissue. The corrosion behavior can be influenced by different factors, among them the grain size, which can be changed by severe plastic deformation processes such as High Pressure Torsion Extrusion (HPTE). This study focuses on the corrosion behavior of samples of pure magnesium and ZK60 before and after HPTE, and the influence of the microstructure on the corrosion activity. The samples are subjected to immersion tests in phosphate buffered saline solution (PBS). The corrosion activity is defined by the emerging hydrogen volume from the corrosion process which is collected and by subsequently observing the resulting sample surfaces. The findings of this study suggest that pure magnesium shows lower corrosion activities than ZK60 and that HPTE processing leads to higher corrosion activities in PBS.
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.