Evidence map›Paper›PMID 38863333›Full record

ArticleACS applied materials & interfaces2024

Capacity Degradation of Zero-Excess All-Solid-State Li Metal Batteries Using a Poly(ethylene oxide) Based Solid Electrolyte.

Philipp Müller, Conrad Szczuka, Chih-Long Tsai, Sandro Schöner, Anna Windmüller, Shicheng Yu, Dominik Steinle, Hermann Tempel, Dominic Bresser, Hans Kungl and 1 more

Abstract read
In one paragraph

Article in ACS applied materials & interfaces, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.

0numbers the graph read from it
0cells of the map it votes in
1citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

1 citing paper in PubMed.

  1. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

11 authors.

Philipp MüllerInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0009-0009-2619-2489
Conrad SzczukaInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.
Chih-Long TsaiInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0001-8103-3514
Sandro SchönerInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0001-6591-9462
Anna WindmüllerInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0003-2829-3362
Shicheng YuInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0002-6619-3330
Dominik SteinleHelmholtz Institute Ulm (HIU), Ulm 89081, Germany.
Hermann TempelInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0002-9794-6403
Dominic BresserHelmholtz Institute Ulm (HIU), Ulm 89081, Germany.ORCID 0000-0001-6429-6048
Hans KunglInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.
Rüdiger-A EichelInstitut für Energie- und Klimaforschung (IEK-9: Grundlagen der Elektrochemie), Forschungszentrum Jülich, Jülich 52425, Germany.ORCID 0000-0002-0013-6325

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Solid-state polymer electrolytes (SPEs), such as poly(ethylene oxide) (PEO), have good flexibility when compared to ceramic-type solid electrolytes. Therefore, it could be an ideal solid electrolyte for zero-excess all-solid-state Li metal battery (ZESSLB), also known as anode-free all-solid-state Li battery, development by offering better contact to the Cu current collector. However, the low Coulombic efficiencies observed from polymer type solid-state Li batteries (SSLBs) raise the concern that PEO may consume the limited amount of Li in ZESSLB to fail the system. Here, we designed ZESSLBs by using all-ceramic half-cells and an extra PEO electrolyte interlayer to study the reactivity between PEO and freshly deposited Li under a real battery operating conduction. By shuttling active Li back from the anode to the cathode, the PEO SPEs can be separated from the ZESSLBs for experimental studies without the influence from cathode materials or possible contamination from the usage of Li foil as the anode. Electrochemical cycling of ZESSLBs shows that the capacities of ZESSLBs with solvent-free and solvent-casted PEO SPEs significantly degraded compared to the ones with Li metal as the anode for the all-solid-state Li batteries. The fast capacity degradation of ZESSLBs using different types of PEO SPEs is evidenced to be associated with Li reacting with PEO, residual solvent, and water in PEO and dead Li formation upon the presence or absence of residual solvent. The results suggest that avoiding direct contact between the PEO electrolyte and deposited lithium is necessary when there is only a limited amount of Li available in ZESSLBs.

Indexed as

anode-freeinterfaceLi anodePEOpolymer electrolytezero-excess

Identifiers

PMID38863333
PMCPMC11212021

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.