ArticleBMC oral health2024
Effect of glazing and thermocycling on the fracture toughness and hardness of a New fully crystallized aluminosilicate CAD/CAM ceramic material.
Ahmed Mahmoud Fouda et al.PubMed ↗Full text ↗Publisher ↗
No numbers read from the abstract.