ArticleMaterials (Basel, Switzerland)2024
Regenerative Superhydrophobic Coatings for Enhanced Performance and Durability of High-Voltage Electrical Insulators in Cold Climates.
Article in Materials (Basel, Switzerland), 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 4 citations in OpenAlex.
- Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
4 authors at 1 institution in 1 country.
Funding
Abstract
Superhydrophobic coatings can be a suitable solution for protecting vulnerable electrical infrastructures in regions with severe meteorological conditions. Regenerative superhydrophobicity, the ability to regain superhydrophobicity after being compromised or degraded, could address the issue of the low durability of these coatings. In this study, we fabricated a superhydrophobic coating comprising hydrophobic aerogel microparticles and polydimethylsiloxane (PDMS)-modified silica nanoparticles within a PDMS matrix containing trifluoropropyl POSS (F-POSS) and XIAMETER PMX-series silicone oil as superhydrophobicity-regenerating agents. The fabricated coating exhibited a static contact angle of 169.5° and a contact angle hysteresis of 6°. This coating was capable of regaining its superhydrophobicity after various pH immersion and plasma deterioration tests. The developed coating demonstrated ice adhesion as low as 71.2 kPa, which remained relatively unchanged even after several icing/de-icing cycles. Furthermore, the coating exhibited a higher flashover voltage than the reference samples and maintained a minimal drop in flashover voltage after consecutive testing cycles. Given this performance, this developed coating can be an ideal choice for enhancing the lifespan of electrical insulators.
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.