ArticleHeliyon2024
C.P titanium/Ti-6Al-4V joint by spark plasma welding: Microstructure and mechanical properties.
Article in Heliyon, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 6 citations in OpenAlex.
- Examination of kinetic components (pressure and time) of spark plasma sintering on the mechanical properties of WC/W FGM.Scientific reports · 2025Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
6 authors at 1 institution in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The welding ability of Ti-6Al-4V alloy is weak due to their two-phase microstructure. On the other hand, friction welding methods lead to significant microstructural changes. In this research, for the first time, pure titanium was successfully joined to the Ti-6Al-4V alloy, without any change in the microstructure and mechanical properties of both alloys, by applying the SPW method. Further, the effects of temperature, pressure, and time of the SPW process on the microstructure and mechanical properties of commercial pure (C.P) titanium joined to the Ti-6Al-4V alloy were investigated. The results indicated that the effect of temperature and pressure on the SPW process was greater than that of time. Further, mechanical properties investigations showed that the yield strength of the joint interface was larger than that of the substrate metal, following which necking and fracture occurred in the pure titanium substrate metal. The alloy (Ti-Ti64) bonded at 800 °C, with a time of 10 min and pressure of 20 MPa, exhibited the superior bonding of 7-9 μm interface thickness, and excellent tensile strength (534 ± 13 MPa) and Vickers micro-hardness (190 ± 5 HV
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.