Study on Thermomechanical Properties and Morphology of an Epoxy Resin Thermally Conductive Adhesive under Different Curing Conditions.

Cheng Zhang, Zhe Xu, Yingxuan Huang, Yuefeng Li, Yang Li, Bobo Yang, Rongrong Hu, Jun Zou, Changran Zheng, Qi Qian

Abstract read
In one paragraph

Article in ACS omega, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.

0numbers the graph read from it
0cells of the map it votes in
0citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

0 citing papers in PubMed.

No citing paper in PubMed yet.

4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

10 authors.

Cheng ZhangSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.
Zhe XuSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.
Yingxuan HuangSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.
Yuefeng LiSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.
Yang LiSchool of Materials Science and Engineering, Shanghai Institute of Technology, Shanghai 201418, China.
Bobo YangSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.ORCID https://orcid.org/0000-0003-1351-947X
Rongrong HuSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.
Jun ZouSchool of Science, Shanghai Institute of Technology, Shanghai 201418, China.ORCID https://orcid.org/0000-0003-4720-2040
Changran ZhengAcademy for Engineering and Technology, Fudan University, Shanghai 200433, China.
Qi QianZhejiang Silanex Technology (Taizhou) Co., Ltd., No 318, Yongyuan Road, Lunan Street, Luqiao District, Taizhou, Zhejiang 318050, China.

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

An epoxy resin thermally conductive adhesive is a type of thermosetting polymer encapsulation material that exhibits comprehensive performance, and the thermomechanical properties of this adhesive vary significantly under different curing conditions. In this paper, spherical alumina was used as a filler for thermal conductivity to prepare an epoxy resin thermal conductivity adhesive using a multistage freezing mixing method. The effects of various curing conditions on the thermal-mechanical properties and fracture morphology of the epoxy resin thermal conductivity adhesive were studied. The results showed that the curing condition of 150 °C/2.5 h significantly improved the performance of the epoxy resin thermally conductive adhesive. Through the shear test of the composite material, the influence of the curing agent on the adhesion of the thermally conductive adhesive under fixed conditions was explored. It was found that the curing agent with a superbranched structure exhibited latent properties and greatly enhanced the toughness of the cured epoxy resin product. Altering the curing conditions increases the shear strength by up to 307%. With the increase in curing temperature and the extension of curing temperature, the glass transition temperature gradually increased from 103.9 to 159.8 °C. The initial decomposition temperature

Identifiers

PMID38497002
PMCPMC10938327

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.