Effect of Different Primers on Shear Bond Strength of Base Metal Alloys and Zirconia Frameworks.

Marco Dederichs, Zaid Badr, Stephanie Viebranz, Steffen Schroeter, Christoph-Ludwig Hennig, Anne-Sophie Schmelzer, Arndt Guentsch

Open access · goldAbstract read
In one paragraph

Article in Polymers, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 2 papers.

0numbers the graph read from it
0cells of the map it votes in
2citing papers in PubMed
1.2field-weighted citation impact, top 28% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

2 citing papers in PubMed, 3 citations in OpenAlex.

  1. Observational
  2. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

7 authors at 2 institutions in 2 countries.

Marco DederichsPoliclinic of Prosthetic Dentistry and Material Science, Center for Dental Medicine, Jena University Hospital, D-07743 Jena, Germany.ORCID 0000-0002-7497-4559
Zaid BadrTechnological Innovation Center, Department of General Dental Sciences, Marquette University School of Dentistry, Milwaukee, WI 53201-1881, USA.ORCID 0000-0002-5638-3288
Stephanie ViebranzPoliclinic of Prosthetic Dentistry and Material Science, Center for Dental Medicine, Jena University Hospital, D-07743 Jena, Germany.ORCID 0000-0003-2362-4724
Steffen SchroeterPoliclinic of Prosthetic Dentistry and Material Science, Center for Dental Medicine, Jena University Hospital, D-07743 Jena, Germany.
Christoph-Ludwig HennigDepartment of Orthodontics, Center for Dental Medicine, Jena University Hospital, D-07743 Jena, Germany.
Anne-Sophie SchmelzerPoliclinic of Prosthetic Dentistry and Material Science, Center for Dental Medicine, Jena University Hospital, D-07743 Jena, Germany.
Arndt GuentschDepartment of Surgical and Diagnostic Sciences, Marquette University School of Dentistry, Milwaukee, WI 53201-1881, USA.ORCID 0000-0001-8989-1441
Jena University Hospital · DEMarquette University · US

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Ensuring a secure bond between a framework structure and layering composite resin veneer is essential for a long-lasting dental restoration. A variety of primer systems are available to facilitate the adhesive bonding. Nevertheless, the growing preference for efficiency and simplicity in dentistry has made the one-bottle universal primers a desirable option. This study aims to compare the effectiveness of universal primers on the shear bond strength (SBS) of base metal alloy (BMA) and zirconia to layering composite resin. Each 160 BMA and zirconia 20 × 10 × 5 mm test specimen was fabricated. Eight different primers (SunCera Metal Primer, Metal Primer Z, Reliance Metal Primer, Alloy Primer, MKZ Primer, Monobond Plus, ArtPrime Plus, and Clearfil Ceramic Primer Plus) were applied to 20 specimens in each group. Subsequently, a 5 × 2 mm composite resin build-up was applied. SBS tests were performed after 24 h of water storage and after thermocycling (25,000 cycles, 5-55 °C). On BMA, after water storage for 24 h, the bond strength values ranged from 26.53 ± 3.28 MPa (Metal Primer Z) to 29.72 ± 2.00 MPa (MKZ Primer), while after thermocycling, bond strength values ranged from 25.19 ± 1.73 MPa (MKZ Primer) to 27.69 ± 2.37 MPa (Clearfil Ceramic Primer Plus). On a zirconia base, after 24 h, the bond strengths values ranged from 22.63 ± 2.28 MPa (Reliance Primer) to 29.96 ± 2.37 MPa (MKZ Primer) and from 23.77 ± 3.86 MPa (Metal Primer Z) to 28.88 ± 3.09 MPa (Monobond Plus) after thermocycling. While no significant difference in bond strength was found between the primers on the BMA base, five primer combinations differed significantly from each other on zirconia (

Indexed as

10-MDPadhesionbase metal alloycompositeprimerzirconia

Identifiers

PMID38475255
PMCPMC10934292
OpenAlexW4391981947

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.