Evidence map›Paper›PMID 38409171›Full record

ArticleNature communications2024

High-strength and crack-free welding of 2024 aluminium alloy via Zr-core-Al-shell wire.

Jun Jin, Shaoning Geng, Leshi Shu, Ping Jiang, Xinyu Shao, Chu Han, Liangyuan Ren, Yuantai Li, Lu Yang, Xiangqi Wang

Abstract read
In one paragraph

Article in Nature communications, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 7 papers.

0numbers the graph read from it
0cells of the map it votes in
7citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

7 citing papers in PubMed.

  1. Article
  2. Article
  3. Millisecond Laser Oblique Hole Processing of Alumina Ceramics.Nanomaterials (Basel, Switzerland) · 2025
    Article
  4. Article
  5. Article
  6. Burst Ultrafast Laser Welding of Quartz Glass.Materials (Basel, Switzerland) · 2025
    Article
  7. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

10 authors.

Jun JinThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Shaoning GengThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China. sngeng@163.com.ORCID http://orcid.org/0000-0003-2742-2038
Leshi ShuThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Ping JiangThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China. jiangping@hust.edu.cn.ORCID http://orcid.org/0000-0002-2466-0690
Xinyu ShaoThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Chu HanThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Liangyuan RenThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Yuantai LiThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Lu YangThe State Key Laboratory of Intelligent Manufacturing Equipment and Technology, School of Mechanical Science and Engineering, Huazhong University of Science & Technology, Wuhan, Hubei, 430074, PR China.
Xiangqi WangJihua Laboratory Testing Center, Ji Hua Laboratory, Foshan, PR China.

Funding

National Natural Science Foundation of China (National Science Foundation of China) 52075201National Natural Science Foundation of China (National Science Foundation of China) 52188102National Natural Science Foundation of China (National Science Foundation of China) 52305467National Natural Science Foundation of China (National Science Foundation of China) U22A20196
6 · The paper itself

Abstract

The 2000 series aluminium alloys are qualified for widespread use in lightweight structures, but solidification cracking during fusion welding has been a long-standing issue. Here, we create a zirconium (Zr)-core-aluminium (Al)-shell wire (ZCASW) and employ the oscillating laser-arc hybrid welding technique to control solidification during welding, and ultimately achieve reliable and crack-free welding of 2024 aluminium alloy. We select Zr wires with an ideal lattice match to Al based on crystallographic information and wind them by the Al wires with similar chemical components to the parent material. Crack-free, equiaxed (where the length, width and height of the grains are roughly equal), fine-grained microstructures are acquired, thereby considerably increasing the tensile strength over that of conventional fusion welding joints, and even comparable to that of friction stir welding joints. This work has important engineering application value in welding of high-strength aluminum alloys.

Identifiers

PMID38409171
PMCPMC10897384

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked