Evidence map›Paper›PMID 38399849›Full record

ArticlePolymers2024

Sustainable Composites: Analysis of Filler-Rubber Interaction in Natural Rubber-Styrene-Butadiene Rubber/Polyurethane Composites Using the Lorenz-Park Method and Scanning Electron Microscopy.

Arthur Pimentel De Carvalho, Harison Franca Dos Santos, Gabriel Deltrejo Ribeiro, Carlos Toshiyuki Hiranobe, Danielle Goveia, Elmer Mateus Gennaro, Leonardo Lataro Paim, Renivaldo José Dos Santos

Open access · goldAbstract read
In one paragraph

Article in Polymers, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.

0numbers the graph read from it
0cells of the map it votes in
1citing papers in PubMed
2.0field-weighted citation impact, top 15% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

1 citing paper in PubMed, 12 citations in OpenAlex.

  1. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

8 authors at 1 institution in 1 country.

Arthur Pimentel De CarvalhoDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.
Harison Franca Dos SantosDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.
Gabriel Deltrejo RibeiroDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.
Carlos Toshiyuki HiranobeDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.ORCID 0000-0002-5182-2018
Danielle GoveiaDepartment of Science and Technology, Institute of Sciences and Engineering, Sao Paulo State University (UNESP), Itapeva 18409-010, SP, Brazil.ORCID 0000-0001-6170-5459
Elmer Mateus GennaroDepartment of Aeronautical Engineering, Engineering School, Sao Paulo State University (UNESP), São João da Boa Vista 13876-750, SP, Brazil.ORCID 0000-0003-1074-396X
Leonardo Lataro PaimDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.ORCID 0000-0002-5113-6376
Renivaldo José Dos SantosDepartment of Engineering, Faculty of Engineering and Science, Sao Paulo State University (UNESP), Rosana 19274-000, SP, Brazil.
Universidade Estadual Paulista (Unesp) · BR

Funding

São Paulo Research Foundation 2020/05549-4
6 · The paper itself

Abstract

This study examined micronized polyurethane residues as a reinforcing filler in elastomeric composites made from natural rubber (NR) and styrene-butadiene rubber (SBR). Due to growing environmental concerns, this research aimed to find sustainable alternatives to synthetic materials. The results indicated that adding micronized polyurethane improved the mechanical properties of the composites, reinforcing the polymer matrix and increasing the cross-link density as a barrier against solvents. The composites met the requirements for industrial applications, though; at 40 phr of polyurethane filler, material deformation was reduced, indicating saturation. FTIR analysis confirmed the homogeneity of the materials without chemical reactions, while electron microscopy revealed an increase in the number of particles and irregularities with the filler. The composite with 10 phr showed a lower volume loss in abrasion resistance, meeting the standards for soles. The composite with 30 phr of polyurethane achieved the best results without the filler's saturation and met the footwear industry's requirements. The results show the potential for sustainable practices in industry using this elastomeric blend.

Indexed as

compositesfiller–rubber interactionLorenz–Parkpolyurethane wasteshoe sole

Identifiers

PMID38399849
PMCPMC10893311
OpenAlexW4391652330

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.