ArticleHeliyon2024
Preparation and characterization of polyvinyl alcohol (PVA)-glycerol composite films incorporating nanosilica from municipal solid waste incinerator bottom ash.
Article in Heliyon, 2024. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 21 citations in OpenAlex.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
6 authors at 2 institutions in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
This study investigates the fabrication of a composite film composed of polyvinyl alcohol (PVA) and glycerol, incorporating nanosilica derived from municipal solid waste incinerator bottom ash (BA). The nanosilica is blended with a PVA film-forming solution containing glycerol as a plasticizer. The composite films are characterized using Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and scanning electron microscopy (SEM). Additionally, thermogravimetric analysis (TGA) is conducted to evaluate the thermal properties, while the mechanical properties are assessed in terms of tensile strength (TS) and elongation at break (EAB). The results indicate that the presence of silica nanoparticles reduces transparency and increases film thickness in the presence of glycerol. Notably, the film containing 1% silica demonstrates a significant enhancement in tensile strength, exhibiting a 50% increase compared to the film without silica. However, higher silica loadings lead to a deterioration in mechanical properties due to silica agglomeration within the polymer matrix. As expected, the presence of silica in the films slightly elevates the degradation temperature.
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.