ArticleBrazilian dental journal2023
Long-term effect of firing protocols on surface roughness and flexural strength of lithium disilicate glass-ceramic.
Article in Brazilian dental journal, 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
3 citing papers in PubMed, 3 citations in OpenAlex.
- Influence of Sintering Parameters on the Mechanical Behaviour of Lithium Disilicate Glass Ceramics: An In-Vitro Study.Journal of functional biomaterials · 2025Article
- Effect of staining techniques and repeated firing cycles on translucency, color and biaxial flexural strength of advanced lithium disilicate containing Virgilite crystals.BMC oral health · 2025Article
- Chemical and microstructural evaluation of dental ceramics before and after multiple firing cycles.Brazilian dental journal · 2025Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
5 authors at 1 institution in 1 country.
Funding
No grant is acknowledged in the PubMed record.
Abstract
This study evaluated the effect of different firing protocols on the surface roughness and flexural strength of CAD/CAM lithium disilicate glass-ceramic (LD) after aging methods. Forty-two LD bars of 16 x 4 x 2 mm (IPS e-max CAD, Ivoclar) were randomly separated into two groups according to firing protocols: Single firing-Staining, glazing, and crystallization in a single step; Multiple firings-Crystallization+First staining+Firing+Second staining+Firing+Glazing+Firing. After protocols, initial surface roughness readings were taken (Surfcorder SE1700, Kosakalab). Samples were then randomly separated into three groups (n=7) according to the aging methods they were submitted: Thermomechanical cycling (TMC, ER System, Erios, 1,200,000 cycles, 0.3 MPa, 2 Hz and 5°C/37°C/55°C, 30 s swell time); Simulated toothbrushing (STB, Pepsodent, MAVTEC, 73,000 cycles), and Control (no aging). Final surface roughness readings were done, and samples were submitted to a three-point bending test (OM100, Odeme Dental Research) and fractographic analysis by scanning electron microscopy (EVO-MA10, ZEISS). Data were analyzed (2-way ANOVA, (α=.05). There was no difference (p>.05) in the flexural strength between the firing protocols, regardless of the aging method. STB decreased the flexural strength of samples submitted to multiple firings, different from control (p<.05). Without aging (Control), before TMC, and after STB, LD had lower surface roughness when submitted to multiple firings than to single firing (p<.05). The firing protocols did not affect the flexural strength or the surface roughness of the lithium disilicate glass-ceramic, even after aging. However, toothbrushing negatively affected the flexural strength and smoothed the surface of the ceramic submitted to multiple firings.