ArticlePloS one2023
Valorization of agro-industrial waste from the cassava industry as esterified cellulose butyrate for polyhydroxybutyrate-based biocomposites.
Article in PloS one, 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Not yet cited in PubMed.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
0 citing papers in PubMed, 2 citations in OpenAlex.
No citing paper in PubMed yet.
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
4 authors at 1 institution in 2 countries.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The aim of this study was to utilize cassava pulp to prepare biocomposites comprising microcrystalline cellulose from cassava pulp (CP-MCC) as a filler and polyhydroxybutyrate (PHB) synthesized in-house by Cupriavidus necator strain A-04. The CP-MCC was extracted from fresh cassava pulp. Next, the CP-MCC surface was modified with butyryl chloride (esterified to CP-MCC butyrate) to improve dissolution and compatibility with the PHB. FTIR results confirmed that the esterified CP-MCC butyrate had aliphatic chains replacing the hydroxyl groups; this substitution increased the solubilities in acetone, chloroform, and tetrahydrofuran. Biocomposite films were prepared by varying the composition of esterified CP-MCC butyrate as a filler in the PHB matrix at 0, 5, 10, 15, 20 and 100 wt%. The results for the 95:5 and 90:10 CP-MCC butyrate biocomposite films showed that esterification led to improvements in the thermal properties and increased tensile strengths and elongations at break. All prepared biocomposite films maintained full biodegradability.