Evidence map›Paper›PMID 37897312›Full record

ArticleAdvanced science (Weinheim, Baden-Wurttemberg, Germany)2023

Breaking the Axis-Symmetry of a Single-Wall Carbon Nanotube During Its Growth.

Lili Zhang, Ziwei Xu, Tian-Liang Feng, Maoshuai He, Thomas Willum Hansen, Jakob Birkedal Wagner, Chang Liu, Hui-Ming Cheng

Open access · goldAbstract read
In one paragraph

Article in Advanced science (Weinheim, Baden-Wurttemberg, Germany), 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 2 papers.

0numbers the graph read from it
0cells of the map it votes in
2citing papers in PubMed
0.9field-weighted citation impact, top 31% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

2 citing papers in PubMed, 9 citations in OpenAlex.

  1. Review
  2. Breaking the Axis-Symmetry of a Single-Wall Carbon Nanotube During Its Growth.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2023
    Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

8 authors at 4 institutions in 2 countries.

Lili ZhangShenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang, 110016, China.ORCID https://orcid.org/0000-0002-5383-8435
Ziwei XuSchool of Materials Science and Engineering, Jiangsu University, Zhenjiang, 212013, China.ORCID https://orcid.org/0000-0002-6143-182X
Tian-Liang FengSchool of Materials Science and Engineering, Jiangsu University, Zhenjiang, 212013, China.
Maoshuai HeCollege of Chemistry and Molecular Engineering, Qingdao University of Science and Technology, Qingdao, 266042, China.ORCID https://orcid.org/0000-0003-4436-8168
Thomas Willum HansenDTU Nanolab, Technical University of Denmark, Fysikvej, Kongens Lyngby, 2800, Denmark.ORCID https://orcid.org/0000-0002-1861-3054
Jakob Birkedal WagnerDTU Nanolab, Technical University of Denmark, Fysikvej, Kongens Lyngby, 2800, Denmark.ORCID https://orcid.org/0000-0002-2945-0190
Chang LiuShenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang, 110016, China.ORCID https://orcid.org/0000-0003-3016-3997
Hui-Ming ChengShenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, 72 Wenhua Road, Shenyang, 110016, China.ORCID https://orcid.org/0000-0002-5387-4241
Chinese Academy of Sciences · CNJiangsu University · CNTechnical University of Denmark · DKQingdao University of Science and Technology · CN

Funding

Chinese Academy of Sciences and the Shenyang National Laboratory for Materials ScienceEuropean Union Seventh Framework Programme (FP7/2007-2013) 604472Key Basic Research Project of Shandong Province, China ZR2019ZD49National Natural Science Foundation of China 51802316National Natural Science Foundation of China 51927803National Natural Science Foundation of China 51972311National Natural Science Foundation of China 52130209National Natural Science Foundation of China 52188101Natural Science Foundation of Liaoning Province, China 2020-MS-009
6 · The paper itself

Abstract

The asymmetrical growth of a single-wall carbon nanotube (SWCNT) by introducing a change of a local atomic structure, is usually inevitable and supposed to have a profound effect on the chirality control and property tailor. However, the breaking of the symmetry during SWCNT growth remains unexplored and its origins at the atomic-scale are elusive. Here, environmental transmission electron microscopy is used to capture the process of breaking the symmetry of a growing SWCNT from a sub-2-nm platinum catalyst nanoparticle in real-time, demonstrating that topological defects formed on the side of a SWCNT can serve as a buffer for stress release and inherently break its axis-symmetrical growth. Atomic-level details reveal the importance of the tube-catalyst interface and how the atom rearrangement of the solid-state platinum catalyst around the interface influences the final tubular structure. The active sites responsible for trapping carbon dimers and providing enough driving force for carbon incorporation and asymmetric growth are shown to be low-coordination step edges, as confirmed by theoretical simulations.

Indexed as

carbon nanotubesenvironmental TEMgrowth mechanisminterface interactionsymmetry breaking

Identifiers

PMID37897312
PMCPMC10754088
OpenAlexW4388001319

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked