Evidence map›Paper›PMID 37896315›Full record

ArticlePolymers2023

Electrode Impact on the Electrical Breakdown of Dielectric Elastomer Thin Films.

Bettina Fasolt, Fabio Beco Albuquerque, Jonas Hubertus, Günter Schultes, Herbert Shea, Stefan Seelecke

Abstract read
In one paragraph

Article in Polymers, 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 4 papers.

0numbers the graph read from it
0cells of the map it votes in
4citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

4 citing papers in PubMed.

  1. Review
  2. Review
  3. Article
  4. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors.

Bettina FasoltIntelligent Material Systems Lab, Center for Mechatronics and Automation Technology, ZeMA gGmbH, DE-66121 Saarbrücken, Germany.ORCID 0000-0002-7117-4839
Fabio Beco AlbuquerqueLMTS Soft Transducers Laboratory, EPFL Ecole Polytechnique Fédérale de Lausanne, CH-2002 Neuchâtel, Switzerland.
Jonas HubertusSensors and Thin Film Group, University of Applied Sciences, DE-66117 Saarbrücken, Germany.
Günter SchultesSensors and Thin Film Group, University of Applied Sciences, DE-66117 Saarbrücken, Germany.
Herbert SheaLMTS Soft Transducers Laboratory, EPFL Ecole Polytechnique Fédérale de Lausanne, CH-2002 Neuchâtel, Switzerland.ORCID 0000-0003-3527-3036
Stefan SeeleckeIntelligent Material Systems Lab, Department of Systems Engineering, Department of Materials Science and Engineering, Saarland University, DE-66121 Saarbrücken, Germany.ORCID 0000-0003-1018-247X

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Dielectric Elastomer Actuators (DEAs) enable the realization of energy-efficient and compact actuator systems. DEAs operate at the kilovolt range with typically microampere-level currents and hence minimize thermal losses in comparison to low voltage/high current actuators such as shape memory alloys or solenoids. The main limiting factor for reaching high energy density in high voltage applications is dielectric breakdown. In previous investigations on silicone-based thin films, we reported that not only do environmental conditions and film parameters such as pre-stretch play an important role but that electrode composition also has a significant impact on the breakdown behavior. In this paper, we present a comprehensive study of electrical breakdown on thin silicone films coated with electrodes manufactured by five different methods: screen printing, inkjet printing, pad printing, gold sputtering, and nickel sputtering. For each method, breakdown was studied under environmental conditions ranging from 1 °C to 80 °C and 10% to 90% relative humidity. The effect of different manufacturing methods was analyzed as was the influence of parameters such as solvents, silicone content, and the particle processing method. The breakdown field increases with increasing temperature and decreases with increasing humidity for all electrode types. The stiffer metal electrodes have a higher breakdown field than the carbon-based electrodes, for which particle size also plays a large role.

Indexed as

carbon blackdielectric breakdown testelectrode manufacturing methodsenvironmental conditionsinfluence electrodessilicone films

Identifiers

PMID37896315
PMCPMC10610327

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.