ArticleMaterials (Basel, Switzerland)2023
Properties of Geopolymers Based on Metakaolin and Soda-Lime Waste Glass.
Article in Materials (Basel, Switzerland), 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 2 papers.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
2 citing papers in PubMed.
- Article
- Geopolymer Concretes with Organic Phase Change Materials-Analysis of Thermal Properties and Microstructure.Materials (Basel, Switzerland) · 2025Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
2 authors.
Funding
No grant is acknowledged in the PubMed record.
Abstract
The paper determines the properties of geopolymer pastes based on metakaolin and soda-lime waste glass. The density, alkaline activity, strength and microstructure of the reference geopolymer, as well as geopolymers with a 10%, 30% and 50% soda-lime waste glass content instead of metakaolin, were tested. The experimental results indicate that the properties of the geopolymers with waste glass largely depend on the ratio of the liquid to solid substance. Increasing the content of waste glass causes an increase in the fluidity of the geopolymer paste, which in turn allows the amount of water glass, i.e., an activator during the obtaining of geopolymers, to be reduced. On the basis of the conducted tests, it was found that the strength of geopolymers can be increased by adding up to 50% of soda-lime waste glass instead of metakaolin and by having a lower content of water glass.