Fast synthesis of large-area bilayer graphene film on Cu.

Jincan Zhang, Xiaoting Liu, Mengqi Zhang, Rui Zhang, Huy Q Ta, Jianbo Sun, Wendong Wang, Wenqing Zhu, Tiantian Fang, Kaicheng Jia and 22 more

Abstract read
In one paragraph

Article in Nature communications, 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 7 papers.

0numbers the graph read from it
0cells of the map it votes in
7citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

7 citing papers in PubMed.

  1. Article
  2. Article
  3. Article
  4. Intelligent self-correcting growth of uniform Bernal-stacked bi-/trilayer graphene.Proceedings of the National Academy of Sciences of the United States of America · 2025
    Article
  5. Article
  6. Article
  7. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

32 authors.

Jincan Zhang *Center for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Xiaoting Liu *Center for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Mengqi Zhang *Beijing Graphene Institute, 100095, Beijing, P. R. China.
Rui Zhang *Department of Physics and Astronomy, University of Manchester, Manchester, M13 9PL, UK.
Huy Q TaLeibniz Institute for Solid State and Materials Research Dresden, P.O. Box 270116, D-01171, Dresden, Germany.
Jianbo SunBeijing Graphene Institute, 100095, Beijing, P. R. China.
Wendong WangDepartment of Physics and Astronomy, University of Manchester, Manchester, M13 9PL, UK.
Wenqing ZhuState Key Laboratory for Turbulence and Complex System, Department of Mechanics and Engineering Science, College of Engineering, Peking University, 100871, Beijing, P. R. China.
Tiantian FangCAS Key Laboratory of Analytical Chemistry for Living Biosystems, Institute of Chemistry, Chinese Academy of Sciences, 100190, Beijing, P. R. China.
Kaicheng JiaCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Xiucai SunCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Xintong ZhangBeijing Graphene Institute, 100095, Beijing, P. R. China.
Yeshu ZhuCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Jiaxin ShaoCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Yuchen LiuBeijing Graphene Institute, 100095, Beijing, P. R. China.
Xin GaoCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Qian YangCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Luzhao SunCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.ORCID http://orcid.org/0000-0003-0518-0744
Qin LiBeijing Graphene Institute, 100095, Beijing, P. R. China.
Fushun LiangCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Heng ChenCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Liming ZhengCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China.
Fuyi WangBeijing National Laboratory for Molecular Sciences, National Centre for Mass Spectrometry in Beijing, CAS Key Laboratory of Analytical Chemistry for Living Biosystems, Institute of Chemistry, Chinese Academy of Sciences, 100190, Beijing, P. R. China.
Wanjian YinSoochow Institute for Energy and Materials Innovations, Soochow University, 215006, Suzhou, P. R. China.ORCID http://orcid.org/0000-0003-0932-2789
Xiaoding WeiState Key Laboratory for Turbulence and Complex System, Department of Mechanics and Engineering Science, College of Engineering, Peking University, 100871, Beijing, P. R. China.ORCID http://orcid.org/0000-0002-5173-4923
Jianbo YinBeijing Graphene Institute, 100095, Beijing, P. R. China.ORCID http://orcid.org/0000-0001-6610-3916
Thomas GemmingLeibniz Institute for Solid State and Materials Research Dresden, P.O. Box 270116, D-01171, Dresden, Germany.ORCID http://orcid.org/0000-0002-7353-595X
Mark H RummeliLeibniz Institute for Solid State and Materials Research Dresden, P.O. Box 270116, D-01171, Dresden, Germany.
Haihui LiuSchool of Material Science and Engineering, Tianjin Key Laboratory of Advanced Fibers and Energy Storage, State Key Laboratory of Separation Membranes and Membrane Processes, Tiangong University, 300387, Tianjin, P. R. China. liuhaihui@tiangong.edu.cn.ORCID http://orcid.org/0009-0000-8481-0059
Hailin PengCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China. hlpeng@pku.edu.cn.ORCID http://orcid.org/0000-0003-1569-0238
Li LinSchool of Materials Science and Engineering, Peking University, 100871, Beijing, P. R. China. linli-cnc@pku.edu.cn.ORCID http://orcid.org/0000-0002-3626-0643
Zhongfan LiuCenter for Nanochemistry, Beijing Science and Engineering Center for Nanocarbons, Beijing National Laboratory for Molecular Science, College of Chemistry and Molecular Engineering, Peking University, 100871, Beijing, P. R. China. zfliu@pku.edu.cn.ORCID http://orcid.org/0000-0001-5554-1902

Funding

National Natural Science Foundation of China (National Science Foundation of China) 51520105003
6 · The paper itself

Abstract

Bilayer graphene (BLG) is intriguing for its unique properties and potential applications in electronics, photonics, and mechanics. However, the chemical vapor deposition synthesis of large-area high-quality bilayer graphene on Cu is suffering from a low growth rate and limited bilayer coverage. Herein, we demonstrate the fast synthesis of meter-sized bilayer graphene film on commercial polycrystalline Cu foils by introducing trace CO

Identifiers

PMID37268632
PMCPMC10238369

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.