Biological and Oxidative Degradation of Ultrathin-Fibrous Nonwovens Based on Poly(lactic Acid)/Poly(3-Hydroxybutyrate) Blends.

Anatoly Aleksandrovich Olkhov, Elena Evgenyevna Mastalygina, Vasily Andreevich Ovchinnikov, Alexander Sergeevich Kurnosov, Anatoly Anatolyevich Popov, Alexey Leonidovich Iordanskii

Open access · goldAbstract read
In one paragraph

Article in International journal of molecular sciences, 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 3 papers.

0numbers the graph read from it
0cells of the map it votes in
3citing papers in PubMed
0.9field-weighted citation impact, top 30% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

3 citing papers in PubMed, 9 citations in OpenAlex.

  1. Review
  2. Review
  3. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors at 3 institutions in 1 country.

Anatoly Aleksandrovich OlkhovScientific Laboratory "Advanced Composite Materials and Technologies", Plekhanov Russian University of Economics, 36 Stremyanny Ln, 117997 Moscow, Russia.ORCID 0000-0003-0615-6914
Elena Evgenyevna MastalyginaScientific Laboratory "Advanced Composite Materials and Technologies", Plekhanov Russian University of Economics, 36 Stremyanny Ln, 117997 Moscow, Russia.ORCID 0000-0002-3684-6521
Vasily Andreevich OvchinnikovScientific Laboratory "Advanced Composite Materials and Technologies", Plekhanov Russian University of Economics, 36 Stremyanny Ln, 117997 Moscow, Russia.
Alexander Sergeevich KurnosovInstitute of Biochemical Physics named after N.M. Emanuel, Russian Academy of Sciences, 4 Kosygin St., 119991 Moscow, Russia.
Anatoly Anatolyevich PopovScientific Laboratory "Advanced Composite Materials and Technologies", Plekhanov Russian University of Economics, 36 Stremyanny Ln, 117997 Moscow, Russia.
Alexey Leonidovich IordanskiiN.N. Semenov Federal Research Center for Chemical Physics, Russian Academy of Sciences, 4 Kosygin St., 119334 Moscow, Russia.ORCID 0000-0003-0771-0825
Plekhanov Russian University of Economics · RUInstitute of Biochemical Physics NM Emanuel · RUSemenov Institute of Chemical Physics · RU

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Developing biodegradable materials based on polymer blends with a programmable self-destruction period in the environmental conditions of living systems is a promising direction in polymer chemistry. In this work, novel non-woven fibrous materials obtained by electrospinning based on the blends of poly(lactic acid) (PLA) and poly(3-hydroxybutyrate) (PHB) were developed. The kinetics of biodegradation was studied in the aquatic environment of the inoculum of soil microorganisms. Oxidative degradation was studied under the ozone gaseous medium. The changes in chemical composition and structure of the materials were studied by optical microscopy, DSC, TGA, and FTIR-spectroscopy. The disappearance of the structural bands of PHB in the IR-spectra of the blends and a significant decrease in the enthalpy of melting after 90 days of exposure in the inoculum indicated the biodegradation of PHB while PLA remained stable. It was shown that the rate of ozonation was higher for PLA and the blends with a high content of PLA. The lower density of the amorphous regions of the blends determined an increased rate of their oxidation by ozone compared to homopolymers. The optimal composition in terms of degradation kinetics is a fibrous material based on the blend of 30PLA/70PHB that can be used as an effective ecosorbent, for biopackaging, and as a highly porous covering material for agricultural purposes.

Indexed as

HydroxybutyratesPolyesters3-Hydroxybutyric AcidOxidative StressPolyhydroxybutyratesPolymers3-Hydroxybutyric AcidHydroxybutyratespoly-beta-hydroxybutyratePolyestersPolyhydroxybutyratespoly(lactide)Polymersbiodegradationelectrospinningnon-woven matrixoxidation by ozonepoly(3-hydroxybutyrate)poly(lactic acid)polymer blendultrathin-fibrous nonwovens

Identifiers

PMID37175689
PMCPMC10178885
OpenAlexW4367320199

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.