ArticleMaterials (Basel, Switzerland)2023
Strengthening Mechanism of Rotary-Forged Deformable Biodegradable Zn-0.45Li Alloys.
Article in Materials (Basel, Switzerland), 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed.
- Enhancing Mechanical and Biodegradation Properties of Zn-0.5Fe Alloys Through Rotary Forging.Materials (Basel, Switzerland) · 2025Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
9 authors.
Funding
Abstract
The use of zinc (Zn) alloys as a biodegradable metal for medical purposes has been a popular research topic. This study investigated the strengthening mechanism of Zn alloys to enhance their mechanical properties. Three Zn-0.45Li (wt.%) alloys with different deformation amounts were prepared by rotary forging deformation. Their mechanical properties and microstructures were tested. A simultaneous increase in strength and ductility was observed in the Zn-0.45Li alloys. Grain refinement occurred when the rotary forging deformation reached 75.7%. The surface average grain size reached 1.19 ± 0.31 μm, and the grain size was uniformly distributed. Meanwhile, the maximum elongation of the deformed Zn-0.45Li was 139.2 ± 18.6%, and the ultimate tensile strength reached 426.1 ± 4.7 MPa. In situ tensile tests showed that the reinforced alloys still broke from the grain boundary. Continuous and discontinuous dynamic recrystallization during severe plastic deformation produced many recrystallized grains. During deformation, the dislocation density of the alloy first increased and then decreased, and the texture strength of the (0001) direction increased with deformation. Analysis of the mechanism of alloy strengthening showed that the strength and plasticity enhancement of Zn-Li alloys after macro deformation was a combination of dislocation strengthening, weave strengthening, and grain refinement rather than only fine-grain strengthening as observed in conventional macro-deformed Zn alloys.