Evaluating the Stability of PLA-Lignin Filament Produced by Bench-Top Extruder for Sustainable 3D Printing.

Siti Aisyah Syazwani Zaidi, Cham Eng Kwan, Denesh Mohan, Shuhaida Harun, Abdullah Amru Indera Luthfi, Mohd Shaiful Sajab

Full text read
In one paragraph

Article in Materials (Basel, Switzerland), 2023. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 4 papers.

0numbers the graph read from it
0cells of the map it votes in
4citing papers in PubMed
–field-weighted citation impact
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

4 citing papers in PubMed.

  1. Review
  2. Article
  3. Article
  4. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

6 authors.

Siti Aisyah Syazwani ZaidiResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.
Cham Eng KwanResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.ORCID 0000-0003-3507-9882
Denesh MohanResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.ORCID 0000-0002-0867-0055
Shuhaida HarunResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.
Abdullah Amru Indera LuthfiResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.ORCID 0000-0002-0503-0503
Mohd Shaiful SajabResearch Center for Sustainable Process Technology (CESPRO), Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi 43600, Selangor, Malaysia.ORCID 0000-0001-8400-8090

Funding

National University of Malaysia GUP-2021-018UKM-YSD Chair for Sustainability UKM-YSD-2021-006
6 · The paper itself

Abstract

As additive manufacturing continues to evolve, there is ongoing discussion about ways to improve the layer-by-layer printing process and increase the mechanical strength of printed objects compared to those produced by traditional techniques such as injection molding. To achieve this, researchers are exploring ways of enhancing the interaction between the matrix and filler by introducing lignin in the 3D printing filament processing. In this work, research has been conducted on using biodegradable fillers of organosolv lignin, as a reinforcement for the filament layers in order to enhance interlayer adhesion by using a bench-top filament extruder. Briefly, it was found that organosolv lignin fillers have the potential to improve the properties of polylactic acid (PLA) filament for fused deposition modeling (FDM) 3D printing. By incorporating different formulations of lignin with PLA, it was found that using 3 to 5% lignin in the filament leads to an improvement in the Young's modulus and interlayer adhesion in 3D printing. However, an increment of up to 10% also results in a decrease in the composite tensile strength due to the lack of bonding between the lignin and PLA and the limited mixing capability of the small extruder.

Indexed as

3D printing filamentbiocompositesbiodegradablelignin

Identifiers

PMID36902909
PMCPMC10004467

What OpenQuestion holds

Textfull text, public
LicenceCC BY
measurements read63
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.