ArticleMaterials (Basel, Switzerland)2022
Analysis of Filler Metals Influence on Quality of Hard-Faced Surfaces of Gears Based on Tests in Experimental and Operating Conditions.
Article in Materials (Basel, Switzerland), 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 3 citations in OpenAlex.
- Quality, Microstructure, and Properties of Metal Alloys.Materials (Basel, Switzerland) · 2023Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
7 authors at 3 institutions in 3 countries.
Funding
Abstract
Hard-facing as a type of the coating depositing is increasingly used today. Physical-chemical-metallurgical characteristics of contact layers in tribo-mechanical systems depend on the operating conditions and the conditions under which the work surfaces were created. That is the reason the influence of the processing procedures and regime, used in the contact surfaces formation, on development of the wear process of contact elements, is being considered ever more. To determine the influence of the hard-facing technology on characteristics of the gears' working surfaces, the experimental investigations were performed on samples hard-faced on the steel for cementation, by varying the filler metals (FM) and the hard-facing regimes. The samples tested were hard-faced by five "hard" and three "soft" filler metals. Experimental investigations included measuring the hard-faced layers' hardness and determination of their microstructure, as well as the wear resistance in the laboratory conditions, on tribometer and on a specially designed device for tests in the real operating conditions of gears. The wear intensity was monitored by the wear trace's width in the laboratory conditions and by the share of the teeth surfaces affected by the destructive pitting in the operating conditions. The results obtained were compared to results of the base metal (BM) tests, which provided the certain conclusions on which filler metal and which welding procedure are the optimal ones for regeneration of the worn teeth surfaces.
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.