ArticlePolymers2022
The Effect of Pore Volume on the Behavior of Polyurethane-Foam-Based Pressure Sensors.
Article in Polymers, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 1 paper.
What it found
Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.
The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.
The trial behind it
Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.
Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.
Who cites it
1 citing paper in PubMed, 11 citations in OpenAlex.
- Article
Corrections and comments
PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.
Authors and funding
6 authors at 1 institution in 2 countries.
Funding
Abstract
In this work, three different polyurethane (PU) foams were prepared by mixing commonly used isocyanate and polyol with different isocyanate indices (1.0:0.8, 1.0:1.0, 1.0:1.1). Then, the prepared polyurethane foam samples were coated by dip-coating with a fixed ratio of nitrogen-doped, bamboo-shaped carbon nanotubes (N-BCNTs) to obtain pressure sensor systems. The effect of the isocyanate index on the initial resistance, pressure sensitivity, gauge factor (GF), and repeatability of the N-BCNT/PU pressure sensor systems was studied. The pore volume was crucial in finetuning the PU-foam-based sensors ability to detect large strain. Furthermore, large pore volume provides suitable spatial pores for elastic deformation. Sensors with large pore volume can detect pressure of less than 3 kPa, which could be related to their sensitivity in the high range. Moreover, by increasing the pore volume, the electrical percolation threshold can be achieved with a minimal addition of nanofillers. On the other hand, PU with a smaller pore volume is more suitable to detect pressure above 3 kPa. The developed sensors have been successfully applied in many applications, such as motion monitoring and vibration detection.
Indexed as
Identifiers
What OpenQuestion holds
Registered trials
Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.