Evidence map›Paper›PMID 36015618›Full record

ArticlePolymers2022

Natural Ageing of PLA Filaments, Can It Be Frozen?

Jaime Orellana-Barrasa, Ana Ferrández-Montero, Begoña Ferrari, José Ygnacio Pastor

Open access · goldAbstract read
In one paragraph

Article in Polymers, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 5 papers.

0numbers the graph read from it
0cells of the map it votes in
5citing papers in PubMed
1.3field-weighted citation impact, top 23% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

5 citing papers in PubMed, 17 citations in OpenAlex.

  1. Article
  2. Article
  3. Article
  4. Article
  5. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

4 authors at 2 institutions in 1 country.

Jaime Orellana-BarrasaCentro de Investigación en Materiales Estructurales (CIME), Universidad Politécnica de Madrid, 28040 Madrid, Spain.
Ana Ferrández-MonteroInstituto de Cerámica y Vidrio (CSIC), Campus de Cantoblanco, 28049 Madrid, Spain.ORCID 0000-0003-3399-1069
Begoña FerrariInstituto de Cerámica y Vidrio (CSIC), Campus de Cantoblanco, 28049 Madrid, Spain.ORCID 0000-0003-3377-6844
José Ygnacio PastorCentro de Investigación en Materiales Estructurales (CIME), Universidad Politécnica de Madrid, 28040 Madrid, Spain.ORCID 0000-0003-3561-5999
Instituto de Cerámica y Vidrio · ESUniversidad Politécnica de Madrid · ES

Funding

Agencia Estatal de Investigación, Ministerio de Ciencia e Innovación, España PID2019-106631GB-C42 & C44Comunidad de Madrid, Spain P2018/NMT-4411 ADITIMAT-CMMinisterio de Educación Cultura y Deporte FPU17/02035
6 · The paper itself

Abstract

The physical ageing of polylactic acid (PLA) is a phenomenon that changes the material's properties over time. This ageing process is highly dependent on ambient variables, such as temperature and humidity. For PLA, the ageing is noticeable even at room temperatures, a process commonly referred to as natural ageing. Stopping the ageing by freezing the material can be helpful to preserve the properties of the PLA and stabilise it at any time during its storage until it is required for testing. However, it is essential to demonstrate that the PLA's mechanical properties are not degraded after defrosting the samples. Four different methods for stopping the ageing (anti-ageing processes) are analysed in this paper-all based on freezing and defrosting the PLA samples. We determine the temperature and ambient water vapor influence during the freezing and defrosting process using desiccant and zip bags. The material form selected is PLA filaments (no bulk material or scaffold structures) printed at 190 °C with diameters between 400 and 550 µm and frozen at -24 °C in the presence or absence of a desiccant. The impact of the anti-ageing processes on PLA's ageing and mechanical integrity is studied regarding the thermal, mechanical and fractographical properties. In conclusion, an anti-ageing process is defined to successfully stop the natural ageing of the PLA for an indefinite length of time. This process does not affect the mechanical properties or the structural integrity of the PLA. As a result, large quantities of this material can be produced in a single batch and be safely stored to be later characterised under the same manufacturing and ageing conditions, which is currently a limiting factor from an experimental point of view as polymeric filament properties can show significant variety from batch to batch.

Indexed as

ageingdesiccantfreezingfused filament fabricationPLAthermal and mechanical properties

Identifiers

PMID36015618
PMCPMC9416607
OpenAlexW4293680860

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials