Evidence map›Paper›PMID 35682779›Full record

ArticleInternational journal of molecular sciences2022

In Vitro Monitoring of Magnesium-Based Implants Degradation by Surface Analysis and Optical Spectroscopy.

Hafiz Wajahat Hassan, Maryam Rahmati, Alejandro Barrantes, Håvard Jostein Haugen, Peyman Mirtaheri

Open access · goldAbstract read
In one paragraph

Article in International journal of molecular sciences, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 6 papers.

0numbers the graph read from it
0cells of the map it votes in
6citing papers in PubMed
1.2field-weighted citation impact, top 25% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

6 citing papers in PubMed, 16 citations in OpenAlex.

  1. Article
  2. Article
  3. Article
  4. Article
  5. Article
  6. A Novel PLLA/MgFMaterials (Basel, Switzerland) · 2023
    Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

5 authors at 2 institutions in 1 country.

Hafiz Wajahat HassanDepartment of Mechanical, Electronic and Chemical Engineering, Faculty of Technology, Art and Design, Oslo Metropolitan University, 0130 Oslo, Norway.ORCID 0000-0002-3499-2218
Maryam RahmatiDepartment of Biomaterials, Institute of Clinical Dentistry and Oral Research Laboratory, University of Oslo, 0317 Oslo, Norway.
Alejandro BarrantesDepartment of Biomaterials, Institute of Clinical Dentistry and Oral Research Laboratory, University of Oslo, 0317 Oslo, Norway.
Håvard Jostein HaugenDepartment of Biomaterials, Institute of Clinical Dentistry and Oral Research Laboratory, University of Oslo, 0317 Oslo, Norway.ORCID 0000-0002-6690-7233
Peyman MirtaheriDepartment of Mechanical, Electronic and Chemical Engineering, Faculty of Technology, Art and Design, Oslo Metropolitan University, 0130 Oslo, Norway.
University of Oslo · NOOsloMet – Oslo Metropolitan University · NO

Funding

European Union 811226
6 · The paper itself

Abstract

Magnesium (Mg)-based degradable alloys have attracted substantial attention for tissue engineering applications due to their biodegradability and potential for avoiding secondary removal surgeries. However, insufficient data in the existing literature regarding Mg's corrosion and gas formation after implantation have delayed its wide clinical application. Since the surface properties of degradable materials constantly change after contact with body fluid, monitoring the behaviour of Mg in phantoms or buffer solutions could provide some information about its physicochemical surface changes over time. Through surface analysis and spectroscopic analysis, we aimed to investigate the structural and functional properties of degradable disks. Since bubble formation may lead to inflammation and change pH, monitoring components related to acidosis near the cells is essential. To study the bubble formation in cell culture media, we used a newly developed Mg alloy (based on Mg, zinc, and calcium), pure Mg, and commercially available grade 2 Titanium (Ti) disks in Dulbecco's Modified Eagle Medium (DMEM) solution to observe their behaviour over ten days of immersion. Using surface analysis and the information from near-infrared spectroscopy (NIRS), we concluded on the conditions associated with the medical risks of Mg alloy disintegration. NIRS is used to investigate the degradation behaviour of Mg-based disks in the cell culture media, which is correlated with the surface analysis where possible.

Indexed as

AlloysMagnesiumCorrosionMaterials TestingMicroscopy, Electron, ScanningSpectrometry, X-Ray EmissionSurface PropertiesAlloysMagnesiumbubble formationdegradation of magnesiumin vitro monitoringoptical spectroscopypartial-least-squares regression

Identifiers

PMID35682779
PMCPMC9181122
OpenAlexW4281741209

What OpenQuestion holds

Textmetadata
LicenceCC BY
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.