Evidence map›Paper›PMID 35647455›Full record

ArticleACS omega2022

Characterization and Performance Testing of an Intumescent Nanoinhibitor for Inhibiting Coal Spontaneous Combustion.

Zhian Huang, Donghong Song, Yinghua Zhang, Yichao Yin, Xiangming Hu, Yukun Gao, Yifu Yang, Ye Tian

Open access · goldAbstract read
In one paragraph

Article in ACS omega, 2022. The graph could read no effect estimate from its abstract, so it casts no vote on the map. Cited by 4 papers.

0numbers the graph read from it
0cells of the map it votes in
4citing papers in PubMed
2.2field-weighted citation impact, top 14% of its field
1 · What the graph read from it

What it found

Each row is one number read from the abstract, on the scale the paper reported it, with its interval. Left of the dashed line favours the treatment, right favours the comparator. Under each row is the sentence it came from. New to these charts? A ten-minute tutorial.

The abstract states no effect estimate the extractor could read, or names no intervention and outcome on the map, so this paper lights no cell and moves no belief. It is still indexed, cited and linked below.

2 · The registry

The trial behind it

Trials whose registry record cites this paper, or whose number appears in the abstract. A trial that started after this paper was published is citing it as background, not reporting it.

Neither the registry nor the abstract names a trial number. If this is a trial report, that itself is worth knowing.

3 · Its place in the literature

Who cites it

4 citing papers in PubMed, 15 citations in OpenAlex.

  1. Article
  2. Article
  3. Article
  4. Article
4 · The record

Corrections and comments

PubMed lists nothing against this paper. Absence here is not a guarantee, only a check that was made.

5 · Who and what money

Authors and funding

8 authors at 3 institutions in 1 country.

Zhian HuangState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.ORCID https://orcid.org/0000-0002-1858-9509
Donghong SongState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.
Yinghua ZhangState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.ORCID https://orcid.org/0000-0003-1129-6938
Yichao YinState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.
Xiangming HuKey Laboratory of Mining Disaster Prevention and Control (Shandong University of Science and Technology), Qingdao, Shandong 266590, China.
Yukun GaoState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.ORCID https://orcid.org/0000-0001-6244-9311
Yifu YangState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.
Ye TianState Key Laboratory of High-Efficient Mining and Safety of Metal Mines (University of Science and Technology Beijing), Ministry of Education, Beijing 100083, China.
University of Science and Technology Beijing · CNHenan Polytechnic University · CNShandong University of Science and Technology · CN

Funding

No grant is acknowledged in the PubMed record.

6 · The paper itself

Abstract

Considering disadvantages such as the low thermal stability and environmental pollution of existing gel inhibitors, a green and stable intumescent nanoinhibitor (INI) was prepared and tested. First, polyacrylamide (PAM), nano-silica, and intumescent flame retardant (IFR) were selected as raw materials. The INI was prepared by nanoparticle modification and cross-linking polymerization. Then, the structure and physical properties of INI were tested by Fourier transform infrared spectroscopy, scanning electron microscopy, and rheological experiments. Meanwhile, the inhibition performance of INI was studied through thermogravimetric analysis-Fourier transfer infrared spectroscopy (TGA-FTIR) analysis. The results suggest that the nanomodification improved the dispersibility of INI particles. The addition of modified nano-silica (MNS) and IFR enhances the strength of the reticular structure, thereby improving the transport convenience and covering ability of the INI gel. At high temperatures, IFR can generate a porous foamed carbon layer that further coats the coal. After INI inhibition treatment, the characteristic temperature and activation energy of coal were significantly improved, and the production of carbon monoxide and carbon dioxide decreased. Hence, irrespective of physical properties, physical inhibition performance, or chemical inhibition performance, INI performed well. Research results can provide valuable references for the preparation and performance study of a coal spontaneous combustion inhibitor.

Identifiers

PMID35647455
PMCPMC9134418
OpenAlexW4280566260

What OpenQuestion holds

Textmetadata
LicenceCC BY-NC-ND
Read underepoch 390

Registered trials

None linked

Read under generation 80e0d062 · epoch 390. Bibliography from PubMed, PubMed Central and OpenAlex; grants from NIH RePORTER; trial links from ClinicalTrials.gov; estimates, votes and beliefs from the OpenQuestion graph.